Fatigue Crack Initiation and Growth in Nanocrystalline Ni at Multiple Length‐Scales
Overview of miniaturized in situ SEM fatigue setup and resultant fatigue crack growth data for nanocrystalline Ni. The presented study focuses on the analysis of fatigue crack growth rate (FCGR) in focused ion beam‐notched microcantilevers prepared from nanocrystalline (NC) Ni as a model material.
Igor Moravcik +7 more
wiley +1 more source
We See That Plastics Are Persistent. But Should We Treat Them Universally as a POP? [PDF]
Maurer-Jones MA, Kalita NK.
europepmc +1 more source
Creep‐Induced Microstructural Evolution in an A2‐B2 Superalloy
A 27.3Ta‐27.3Mo‐27.3Ti‐8Cr‐10Al (at.%) refractory high‐entropy alloy with precipitation‐strengthened A2‐B2 microstructure was studied by creep tests at 1030°C, which demonstrate a transition in deformation mechanisms in the range of 100–150 MPa applied stress. This is associated with changes in dislocation–precipitate interactions. Relevant deformation
Liu Yang +10 more
wiley +1 more source
Atomically precise catalysts design toward efficient waste plastic hydrogenolysis. [PDF]
Zhang Z +8 more
europepmc +1 more source
Influence of Test Temperature and Test Frequency on Fatigue Life of Aluminum Alloy EN AW‐2618A
The influence of test temperature and test frequency on the fatigue life of EN AW‐2618A is investigated. High‐cycle fatigue tests are performed at different test temperatures and frequencies on the 1000 h/230°C overaged state. Both test parameters reduce fatigue life due to time‐dependent damage mechanisms.
Ying Han +5 more
wiley +1 more source
Models aproximats per a l'impacte de baixa energia de materials plàstics
Aquest projecte s’ha dut a terme per aprofundir l’estudi sobre els materials polimèrics i el seu comportament davant impacte. Aquest treball estudia el fenomen de la flexió en impacte quan un dard de capçal semiesfèric impacta una proveta de plàstic ...
García Escobar, Manel
core
Plastics and Sustainable Development - Identifying and Quantifying Ecodesign Strategies for Plastics. [PDF]
Venkatachalam V +5 more
europepmc +1 more source
Do not let thermal drift and instrument artifacts deceive high‐temperature nanoindentation results. We compare classical Oliver–Pharr and automatic image recognition analyses across steels and a Ni alloy to quantify these effects. Accounting for artifacts reveals systematic softening with temperature, while Cr and Ni additions boost resistance ...
Velislava Yonkova +2 more
wiley +1 more source
A Tiered Multi-Technique Decision-Support Framework for Contaminant Screening and Recycling-Route Assignment of Mixed Plastic Waste. [PDF]
Chen A, Saxena S, Samaras VG, Dally B.
europepmc +1 more source
Creep Properties and Deformation Mechanism of Additively Manufactured NiAl‐CrMo Composites
Additively manufactured NiAl‐CrMo composites contain numerous interfaces and cell boundaries that control their creep response. At 700°C under high applied stress, creep is dominated by dislocation‐controlled power‐law mechanisms. At 800°C–900°C and lower stresses, creep is primarily diffusion‐controlled along cell boundaries.
Jan Vollhüter +9 more
wiley +1 more source