Results 151 to 160 of about 4,597 (209)
Synthesis of large mordenite crystals with different aspect ratios [PDF]
Large mordenite crystals hold interest for fundamental research on separation and catalysis as well as emerging applications such as functional devices. A number of methods are now available to obtain large mordenite crystals. However, it still remains a
Petra de Jongh, K P de Jong
exaly +2 more sources
Some of the next articles are maybe not open access.
Related searches:
Related searches:
Infrared Study of Acetophenone Adsorption on Mordenite and Dealuminated Mordenite
Journal of Colloid and Interface Science, 1998Infrared spectra of acetophenone adsorbed on mordenite and acid-leached mordenite are reported. The effects of dealumination were characterized by pyridine adsorption and 29Si and 27Al magic angle spinning nuclear magnetic resonance spectroscopy (MAS NMR).
, Ahmad +3 more
openaire +2 more sources
Partial Oxidation of Methane Catalyzed by H-Mordenite and Fluorinated Mordenite
Applied Catalysis, 1988Abstract Mordenite and fluorinated mordenite are compared as catalysts for the partial oxidation of methane in the temperature range 350–425°C. With both catalysts the major product is ethylene but the latter catalyst yields higher conversions up to 425°C at which temperature carbon monoxide and carbon dioxide become the primary products. Eliminating
S. Kowalak, J.B. Moffat
openaire +1 more source
Hydrogen mordenite and hydronium mordenite. Ion exchange and thermal stability
Journal of the Chemical Society, Faraday Transactions 1: Physical Chemistry in Condensed Phases, 1975Isotherms for the Na+⇌ H3O+ exchange in mordenite showed irreversibility. Hydronium mordenite prepared from the Na-form could be fully re-converted to the Na-form with aqueous NaCl, NaOH or CH3COONa, but hydronium mordenite made by heating the NH4-form to 450°C and subsequent hydration underwent only ∼70 % exchange to the Na-form.
Richard M. Barrer, Jacek Klinowski
openaire +1 more source
Enhanced benzene formation on Pt/H-mordenite and Pd/H-mordenite
Catalysis Letters, 1993The distribution of methylcyclopentane (MCP) ring enlargement (RE) products between benzene (Bz) and cyclohexane (CH) provides information on the reaction mechanism. The Bz/CH ratio is in excess of the calculated and experimentally determined equilibrium ratio.
Bruce A. Lerner +2 more
openaire +1 more source
tert-Butylation of toluene over mordenite and cerium-modified mordenite catalysts
Applied Catalysis A: General, 2006Abstract tert -Butylation of toluene with tert -butanol in the liquid phase was studied over large pore mordenite zeolite catalyst (H-MOR CBV 21A with Si/Al = 10.5) and over cerium-modified parent zeolite with 1–6 wt.% of cerium. The catalytic activity and para -selectivity of parent and cerium-modified H-mordenite catalysts is discussed.
G. Kostrab +6 more
openaire +1 more source
Multiple Equilibrium Analysis Description of Adsorption on Na−Mordenite and H−Mordenite
Journal of the American Chemical Society, 1999Adsorption isotherms are reported for Na−mordenite and H−mordenite at several temperatures with a series of gas adsorptives above their critical temperature. The data sets are analyzed with the multiple equilibrium analysis (MEA) method [Drago, R. S.; et al. J. Am. Chem. Soc. 1998, 120, 538−547. Drago, R. S.; et al. J. Phys. Chem.
Charles Edwin Webster +2 more
openaire +1 more source
Journal of the Chemical Society, Faraday Transactions 1: Physical Chemistry in Condensed Phases, 1974
Ion-exchange isotherms have been measured for synthetic mordenite involving the cation pairs Na+⇌Cs+, NH+4⇌K+, NH+4⇌Na+, NH+4⇌Li+, 2NH+4⇌Ca2+, 2NH+4⇌Sr2+ and 2NH+4⇌Ba2+. In all cases except those involving Ca2+ and Sr2+ reversible exchange was effected.
Richard M. Barrer, Jacek Klinowski
openaire +1 more source
Ion-exchange isotherms have been measured for synthetic mordenite involving the cation pairs Na+⇌Cs+, NH+4⇌K+, NH+4⇌Na+, NH+4⇌Li+, 2NH+4⇌Ca2+, 2NH+4⇌Sr2+ and 2NH+4⇌Ba2+. In all cases except those involving Ca2+ and Sr2+ reversible exchange was effected.
Richard M. Barrer, Jacek Klinowski
openaire +1 more source
Dehydration of methylbutanols on mordenites
Bulletin of the Academy of Sciences of the USSR Division of Chemical Science, 19841. Dehydration of 2-methyl-2-butanol takes place on weak and strong acid sites, while 3-methyl-2-butanol is primarily dehydrated on the strong acid sites of the catalyst. 2. Dehydration of 2-methyl-2-butanol on mordenites takes place only according to the mechanism of Β-elimination, while 3-methyl-2-butanol is dehydrated according to the
Kh. M. Minachev +4 more
openaire +1 more source
Diffusion of hydrocarbons in mordenite and molecular-sieve selectivity of mordenite catalysts
Reaction Kinetics and Catalysis Letters, 1979The diffusion of n-octane and n-propylbenzene in mordenite and the molecularsieve selectivity in hydrocracking of octane-propylbenzene binary mixtures over a mordenite catalyst have been studied. The hydrocarbon diffusivities and molecular-sieve selectivity change are accounted for by diffusion through mordenite channel mouths poisoned with an easily ...
openaire +1 more source