Nucleation and growth of mullite whiskers from lanthanum-doped aluminosilicate melts
Nucleation and growth of mullite whiskers in the La2O3-Al2O3-SiO2 system were investigated in the 1500degrees-1700degreesC temperature range. A differential thermal analysis (DTA) showed that the mullitization temperature decreases from 1350degreesC to ...
Magalhaes, WLE +4 more
core +1 more source
Hierarchically structured aluminum borate whisker aerogel via sol–gel method and in-situ reaction
Ultralight, thermally insulating, and temperature-resistant inorganic aerogels, including particulate and fibrous aerogels, serve as excellent thermal protection materials and hold significant applications in aerospace, energy, and environmental ...
Xin Tao +6 more
doaj +1 more source
Ammonia-leaching residues of roasted molybdenite concentrates are intractable wastes and are mostly stockpiled in factories. Common treatments suffer from low Mo recovery and secondary pollution. This study has developed a synergistic process involving a
Guihong Han +6 more
doaj +1 more source
Research on Intelligent Additive Manufacturing of Mullite Whiskers
Abstract Mullite whiskers exhibit exceptional properties such as mechanical durability, oxidative stability, low thermal expansion coefficient, high-temperature tolerance, and excellent thermal shock resistance, making them widely used in aerospace, mechanical manufacturing, and other fields.
Wenkai Wen +5 more
openaire +1 more source
Oxidation of SiC-Whisker/Mullite Composites in Dry Air
Oxidation behavior of mullite composites containing 10 to 30vol% of SiC-whisker (SiC-w) has been studied at 1300°C in dry air. As the volume fraction of SiC-w increased, the weight gain increased. The weight gain curve obeyed the parabolic law for the SiC-w content of 10vol% and at the oxidation time shorter than 200h.
NAKAMURA, Kazuo +3 more
openaire +2 more sources
Preparation of mullite whiskers from kaolinite using CuSO4 as fluxing agent
Mullite whiskers were produced by firing of kaolin at 1400degrees-1550degreesC. CuSO4 was used as fluxing agent. Before firing, spray drying and baking with flour and leaven were employed to give free space to the powders.
Agathopoulos, S. +3 more
core
Fabricação de esponjas cerâmicas à base de mulita e avaliação de seu desempenho em queimadores porosos radiantes [PDF]
Dissertação [mestrado) - Universidade Federal de Santa Catarina, Centro Tecnológico, Programa de Pós-Graduação em Engenharia Mecânica, Florianópolis, 2013.Visando a aplicação em queimadores porosos radiantes, esponjas cerâmicas de mulita com porosidade ...
Rosário, Jefferson Jean do
core
Anisotropic grain growth of mullite
In this report, mullite ceramics with anisotropic grains were attained from a mixture containing aluminum oxide (Al2O3) and silica (SiO2) from high-energy ball milling.
Rahim, Nor Fazlan
core
87th Annual Meeting of the Meteoritical Society 2025: Abstracts
Meteoritics &Planetary Science, Volume 60, Issue S1, Page 30-350, August 2025.
wiley +1 more source
The arc plasma melting technique is a simple method to synthesize high temperaturereaction composites. In this study, mullite-zirconia composite was synthesized by transferred andnon-transferred arc plasma melting, and the results were compared.
A. I. Y. TOK +4 more
core +1 more source