Results 181 to 190 of about 2,010 (256)

Filling a Gap in Materials Mechanics: Nanoindentation at High Constant Strain Rates up to 105 s−1

open access: yesSmall, EarlyView.
A piezoelectric nanoindentation platform enables constant strain‐rate testing up to 105 s−1, extending experimental capabilities to extreme deformation regimes. Distinct hardness upturns are revealed across crystalline and amorphous materials, verified as intrinsic responses through quasi‐static reloading.
Lalith Kumar Bhaskar   +14 more
wiley   +1 more source

Additive Manufacturing of Hot‐Work Tool Steel by In Situ Alloying Using Laser Powder Bed Fusion and Directed Energy Deposition—Strategies to Improve Chemical Homogeneity

open access: yessteel research international, EarlyView.
To support future alloy development a powder mixture is processed by laser additive manufacturing. The powder mixture containing Mo‐ and W‐rich tracers is processed by powder bed fusion using single and double laser exposure and by directed energy deposition which provides drastically enlarged melt pools.
Felix Großwendt   +2 more
wiley   +1 more source

Designing Superlubricious Hydrogels from Spontaneous Peroxidation Gradients. [PDF]

open access: yesACS Appl Mater Interfaces, 2023
Chau AL   +3 more
europepmc   +1 more source

In Situ Alloying of H13 Tool Steel With TiC via PBF‐LB/M

open access: yessteel research international, EarlyView.
H13 tool steel is in situ alloyed with titanium carbides (TiC) in amounts up to 30 wt.%. This approach offers the advantage that the carbides melt only partially during processing, preventing excessive carbon enrichment of the steel matrix. The resulting microstructure consists of coarse, undissolved and fine, reprecipitated carbides, leading to grain ...
Oliver Bürgi   +2 more
wiley   +1 more source

Unlocking Sustainable-by-Design Li-Metal Batteries by Recycled PVB in Blend Polymer Electrolytes. [PDF]

open access: yesChemSusChem
Patriarchi A   +7 more
europepmc   +1 more source

Assessing the microstructure of simple rhamphothecae in chickens (Aves: Galliformes: Gallus gallus domesticus)

open access: yesJournal of Anatomy, EarlyView.
Simple rhamphotheca are externally homogeneous but internally are composed of several corneous layers with varying hardness. Areas under more mechanical stress such as the rostral portion and the tomia are significantly harder than other areas. Abstract Corneous sheaths on the jaws of beaked tetrapods, or rhamphothecae, are classified as simple or ...
Khanh H. T. To   +2 more
wiley   +1 more source

A proximodistal gradient in bone structure and mechanics in the wings of Seba's short‐tailed bat, Carollia perspicillata

open access: yesThe Anatomical Record, Volume 309, Issue 5, Page 1422-1432, May 2026.
Abstract Bats possess the remarkable ability to fly, and with this, distinctive wing bone properties. We investigated the structural, mechanical, and compositional properties of the humerus, radius, metacarpals, and proximal and middle phalanges of Carollia perspicillata, an approximately 15 g fruit‐eating bat native to the Neotropics.
Xiaoxiang Ma   +4 more
wiley   +1 more source

Unusual Swelling Behavior of Hydrogels Modified with Spiropyran as Appendage or Crosslinker

open access: yesAdvanced Functional Materials, Volume 36, Issue 27, 2 April 2026.
Not so innocent after all—spiropyran crosslinkers in methylenebisacrylamide‐crosslinked poly(acrylamide‐co‐acrylic acid) hydrogels increase crosslinking density, but also, counterintuitively, increase swelling. Charge complexation, cooperative chemo‐mechanical effects, and aggregation may explain these observations.
Michael M. Lerch   +7 more
wiley   +1 more source