Results 61 to 70 of about 4,091,571 (176)

Improved high-temperature-strength nickel-base superalloy [PDF]

open access: yes, 1969
Nickel-base superalloy has a strength of 20,000 psi at 2,200 degrees F, approximately double the strength of the strongest available cast nickel-base alloys. It is not subject to the formation of embrittling phases upon long time exposure at intermediate
Waters, W. J., Freche, J. C.
core  

Assessment, analysis and optimization for high temperature sliding wear process parameter with additive built nickel base superalloy

open access: yesMaterials Research Express
Superalloys are highly demanding alloy for high temperature application. The conventional production process and metallurgical sustainability of the superalloy against the applications is the preamble of the existing research.
S P Jani   +4 more
doaj   +1 more source

Physics‐Informed Generative Machine Learning for Designing Crack‐Free γ′‐Strengthened Ni‐Based Superalloys for Laser Powder Bed Fusion

open access: yesMaterials Genome Engineering Advances, Volume 4, Issue 4, October 2026.
This research proposes a physics‐informed generative machine learning framework to design SHA800, a crack‐free γ′‐strengthened nickel‐based superalloy for laser powder bed fusion, achieving a 43% γ′ volume fraction and 587 HV0.2 hardness. ABSTRACT Fabricating γ′‐strengthened nickel‐based superalloys via laser powder bed fusion (LPBF) faces significant ...
Kai Guo   +11 more
wiley   +1 more source

Nickel Base Superalloy Turbine Disk [PDF]

open access: yes, 2005
A low solvus, high refractory alloy having unusually versatile processing mechanical property capabilities for advanced disks and rotors in gas turbine engines.
Gauda, John   +3 more
core  

Restoration and Thermal Stability Investigation of Intermetllic Phase in Exposed Nickel Base Superalloy Udimet 500 Turbine Blades [PDF]

open access: yesMetalurgija, 2007
The Udimet 500 nickel base superalloy blade exposed for 50000 hours in land base gas turbine working conditions faced the structure degradation. Six different heat treatments procedures have been applied (the blades were exposed at 900 °C and 1000 °C for
Wangyao, P.   +4 more
doaj  

AlloyDesignClaw: Optimizing Castability and Mechanical Properties of Nickel‐Based Superalloys

open access: yesMaterials Genome Engineering Advances, Volume 4, Issue 4, October 2026.
A stepwise optimization method is proposed for castability and mechanical properties of nickel‐based superalloys, enabling interpretable dimensionality reduction and efficient multi‐objective optimization of the composition space. An alloy design multi‐agent framework was further developed, integrating large language models, CALPHAD calculation ...
Jiaxuan Ma   +7 more
wiley   +1 more source

Developments in advanced high temperature disc and blade materials for aero-engine gas turbine applications

open access: yes, 2012
The research carried out as part of this EngD is aimed at understanding the high temperature materials used in modern gas turbine applications and providing QinetiQ with the information required to assess component performance in new propulsion systems ...
Everitt, S.
core   +1 more source

Creep fracture of a nickel base single crystal superalloy along [011] orientation

open access: yes工程科学学报, 2015
The creep fracture behavior of a[011] oriented single crystal nickel base superalloy was investigated in the temperature range of 750 to 980℃ and the stress scope of 200 to 680 MPa.
SHUI Li, HU Zhuang-qi
doaj   +1 more source

In‐Situ Construction of Multi‐Scale Heterogeneous Structures in L‐DED IN718 Coatings via WMoTaNb Incorporation for Enhanced Strength‐Toughness Synergy

open access: yesRare Metals, Volume 45, Issue 10, October 2026.
ABSTRACT To improve the strength–toughness balance of IN718, and alleviate the brittleness commonly associated with refractory high‐entropy alloys, this study proposes a novel strategy to fabricate defect‐free IN718/WMoTaNb heterogeneous multiprincipal element alloy coatings via laser‐directed energy deposition.
Zhao Wang   +7 more
wiley   +1 more source

Strain‐Dependent Evolution of Fatigue and Oxidation Damage in a Nickel‐Based Single‐Crystal Superalloy: The Dominant Mechanism Under Low‐Cycle and Thermomechanical Fatigue

open access: yesRare Metals, Volume 45, Issue 10, October 2026.
ABSTRACT Systematic studies on the fatigue deformation and damage mechanisms of nickel‐based single‐crystal superalloys (Ni‐SXs) under combined thermal and mechanical conditions remain limited, particularly regarding the influence of strain amplitude on the relative contributions of fatigue and oxidation damage.
Liyin Zhang   +7 more
wiley   +1 more source