Results 151 to 160 of about 24,512 (259)

Secondary arm coarsening and microsegregation in superalloy PWA-1480 single crystals: Effect of low gravity [PDF]

open access: yes
Single crystal specimens of nickel base superalloy PWA-1480 were directionally solidified on ground and during low gravity (20 sec) and high gravity (90 sec) parabolic maneuver of KC-135 aircraft.
Curreri, P. A.   +3 more
core   +1 more source

Longitudinal shear behavior of several oxide dispersion strengthened alloys [PDF]

open access: yes
Two commercial oxide dispersion strengthened (ODS) alloys, MA-753 and MA-754, and three experimental ODS alloys, MA-757E, MA-755E, and MA-6000E, were tested in shear at 760 C. Comparisons were made with other turbine blade and vane alloys. All of the ODS
Glasgow, T. K.
core   +1 more source

Implementation of Passing Vehicle Search Algorithm for Optimization of WEDM Process of Nickel-Based Superalloy Waspaloy. [PDF]

open access: yesNanomaterials (Basel), 2022
Chaudhari R   +6 more
europepmc   +1 more source

Finite element thermo-viscoplastic analysis of aerospace structures [PDF]

open access: yes
The time-dependent thermo-viscoplastic response of aerospace structures subjected to intense aerothermal loads is predicted using the finite-element method. The finite-element analysis uses the Bodner-Partom unified viscoplastic constitutive relations to
Dechaumphai, Pramote   +2 more
core   +1 more source