Corrosion Inhibition of S275 Carbon Steel in CO2 Capture Systems Using Monoethanolamine (MEA) Solvent

open access: yesMaterials and Corrosion, EarlyView.
Corrosion inhibitors CuSO4 and NaVO3 achieved up to 98% inhibition efficiency for carbon steel S275 in CO2‐loaded MEA solvent, reducing corrosion rates to 9.4 µm/year—outperforming costly stainless steel SS 316 L at a fraction of the cost. ABSTRACT Corrosion in CO2 capture units significantly impacts safety and costs.
Eleni Lamprou   +6 more
wiley   +1 more source

Pitting Corrosion of Hot-Dip Galvanized Coatings. [PDF]

open access: yesMaterials (Basel), 2020
Królikowska A, Komorowski L, Bonora PL.
europepmc   +1 more source

Corrosion Performance of Steel and Zinc‐Based Materials in Diverse Unsaturated Soils: Insights From a 2‐Year Field Exposure

open access: yesMaterials and Corrosion, EarlyView.
The present study generated the corrosion performance of C‐steel, zinc, and galvanized steel in different global unsaturated soil environments for 2 years. Acceptable matching was observed between corrosion rates and identified corrosion products. To properly predict soil corrosion, the results showed that DIN 50929 should include a drainage‐capability
Abdelkader Meroufel   +4 more
wiley   +1 more source

Improved Corrosion Resistance of a Micro‐Alloyed Carbon Steel Assessed by Multi‐Element Electrical Resistance Probes and Coupons in Natural Seawater and Soil

open access: yesMaterials and Corrosion, EarlyView.
Multi‐element electrical resistance probes fabricated from industrial carbon steels enable real‐time corrosion monitoring in natural seawater and soil. A micro‐alloyed grade (AMLoCor) demonstrates up to 2.4 times improved uniform corrosion resistance over conventional S355 GP steel.
Erwan Diler, Johan Becker, Thomas Urios
wiley   +1 more source

Deep Learning Approach for Pitting Corrosion Detection in Gas Pipelines. [PDF]

open access: yesSensors (Basel)
Malashin I   +10 more
europepmc   +1 more source

Analysis of Corrosion and Wall Perforation in the Heat Exchanger Made of AISI 316L Stainless Steel

open access: yesMaterials and Corrosion, EarlyView.
Elevated passivation temperature is identified as the dominant factor triggering localized corrosion and subsequent perforation of AISI 316L heat exchanger tubes. Electrochemical and complementary characterization results show that the alloy retains high resistance to general, pitting, and intergranular corrosion, indicating that failure primarily ...
Bojana Radojković   +7 more
wiley   +1 more source

Microstructural and Electrochemical Study: Pitting Corrosion Mechanism on A390 Al-Si Alloy and Ce-Mo Treatment as a Better Corrosion Protection. [PDF]

open access: yesMaterials (Basel)
Herrera Hernández H   +6 more
europepmc   +1 more source

Multi‐Method Investigation of Intergranular Corrosion of the Aluminium Alloy EN AW‐2024 With Different Cooling Rates After Solution Heat Treatment—Metallography and Eddy Current Testing

open access: yesMaterials and Corrosion, EarlyView.
The corrosion resistance of heat‐treatable aluminium alloys depends directly on the applied heat treatment. This article discusses the relationship between cooling rate and intergranular corrosion sensitivity. The intergranular corrosion depths were determined by light microscopy of cross‐sections and correlated with both non‐destructive eddy current ...