Combined Process‐ and Phase‐Field‐Simulation to Predict the Microstructure of Single‐Crystal Ni‐Based Superalloys

open access: yesAdvanced Engineering Materials, EarlyView.
A combined finite element and phase‐field approach predicts the evolution of microstructure during the directional solidification of Ni‐based superalloys. The model reveals how withdrawal rate, temperature gradient, and wall thickness control the dendrite spacing, highlighting the strong effect of surface regions in thin sections where dendrite growth ...
Sean Böhm   +3 more
wiley   +1 more source

Hot isostatic pressing of single-crystal nickel-base superalloys: Mechanism of pore closure and effect on Mechanical properties

open access: yesMATEC Web of Conferences, 2014
Pore annihilation was investigated in the single-crystal nickel-base superalloy CMSX-4. HIP tests at 1288 °C/103 MPa were interrupted at different times, then the specimens were investigated by TEM, metallography and density measurements. The kinetics of
Epishin Alexander I.   +4 more
doaj   +1 more source

Research progress in effect of Ru on solidification characteristics, precipitation of topologically close-packed phases and creep property of nickel-based single crystal superalloy

open access: yesCailiao gongcheng, 2022
Nickel-based single crystal superalloys are widely used for hot components of advanced turbine engines due to their excellent mechanical properties at elevated temperature.
CAO Kaili   +7 more
doaj   +1 more source

Low‐Angle Grain Boundaries and Re‐Segregation in Single‐Crystalline Ni‐Base Superalloys

open access: yesAdvanced Engineering Materials, EarlyView.
This work demonstrates that Re‐segregation at low‐angle grain boundaries (LAGBs) in Ni‐base superalloys is influenced by misorientation angle. Advanced microscopy and atom probe tomography reveal that higher misorientation angles increases Re‐segregation.
Alireza B. Parsa   +9 more
wiley   +1 more source

Orientation controlling of Ni-based single-crystal superalloy by a novel method: grain selection assisted by un-melted reused seed

open access: yesJournal of Materials Research and Technology, 2019
A new grain selection method assisted by un-melted short seed was proposed to control the primary and secondary orientations of Ni-based single-crystal superalloy.
Wenchao Yang   +5 more
doaj   +1 more source

Productivity‐Driven Optimization of Laser Powder Bed Fusion Parameters for IN718 Superalloy: Process Control, Microstructure, and Mechanical Properties

open access: yesAdvanced Engineering Materials, EarlyView.
This study demonstrates how optimizing laser power, scanning speed, and hatching distance in laser powder bed fusion can boost the productivity of Inconel 718 manufacturing by up to 29% while maintaining mechanical integrity. The work delivers a validated process window and cost–time analysis, offering industry‐ready guidelines for efficient additive ...
Amir Behjat   +7 more
wiley   +1 more source

Effect of oblique angle on the formability, crystal growth behavior and microstructure in laser direct energy deposited thin-wall structure of single-crystal superalloy

open access: yesJournal of Materials Research and Technology
Laser directed energy deposition process shows a tremendous potential to additively repair and manufacture single-crystal components in a near-net shape. For the specific non-vertical structure such as the tilted and torsional sidewalls of single-crystal
Zhaoyang Liu   +5 more
doaj   +1 more source

Rafting of Ni‐Based Superalloys Under Multiaxial Load as Understood by Phase‐Field Simulations and Critical Experiments

open access: yesAdvanced Engineering Materials, EarlyView.
Phase‐field simulations coupled with dislocation‐density‐based crystal plasticity modeling reproduce γ′ rafting behavior in single‐crystal Ni‐based superalloys under varied loading conditions. The model captures both macroscopic creep and microscopic morphology evolution, with results matching high‐temperature creep experiments.
Micheal Younan   +5 more
wiley   +1 more source

Influence of Environment on Creep Properties of MC2 Single Crystal Superalloy at 1150°C [PDF]

open access: yes, 2004
In order to reveal the effect of oxidation on thin blade walls, a new machine allowing tests up to 1250°C under controlled atmosphere has been designed.
Andrieu, Eric   +4 more
core   +1 more source

Parameter Variation in Planetary Ball Milling of Titanium Aluminide Powder in XHV‐Adequate Atmosphere

open access: yesAdvanced Engineering Materials, EarlyView.
This study investigates the effects of milling parameters, including rotational speed, milling duration, and ball‐to‐powder ratio, on TiAl particle size and morphology in an XHV‐equivalent atmosphere. The creation of oxide‐free surfaces enhances the mechanical properties of green bodies.
Jytte Möckelmann   +4 more
wiley   +1 more source