Results 11 to 20 of about 617,177 (261)

A method for increasing the supersolvus critical strain for recrystallization in single-crystal superalloys

open access: yesMaterials Research Letters, 2023
Recrystallization, possibly triggered during heat treatments by plastic strains of only 1–2%, is highly deleterious to Ni-based single-crystal superalloys.
Sicong Lin   +3 more
doaj   +2 more sources

Application of Hot Isostatic Pressing in Nickel-Based Single Crystal Superalloys

open access: yesCrystals, 2022
Hot isostatic pressing (HIP) technology can effectively reduce microstructure defects such as micropores, which are formed during solidification and hominization heat treatment, and thus further improve the high temperature performance of nickel-based SX
Yunsong Zhao, Siliang He, Longfei Li
doaj   +2 more sources

Composition rules of Ni-base single crystal superalloys and its influence on creep properties via a cluster formula approach. [PDF]

open access: yesSci Rep, 2020
The present work investigated the composition evolution of the TMS series of Ni-base single crystal (SC) superalloys in light of the cluster formula approach systematically. The cluster formula of SC superalloys could be expressed with [Al¯-Ni¯12](Al¯,Cr¯
Chen C, Wang Q, Dong C, Zhang Y, Dong H.
europepmc   +2 more sources

Effects of TCP and creep cavity on creep life in the rafting regime for Ru-containing Nickel-based single crystal superalloys

open access: yesMaterials Research Letters, 2023
Ru is crucial in improving creep properties in Nickel-based single-crystal superalloys. The effect of Ru content on the creep behavior of nickel-based single-crystal superalloy was studied.
Y. Zhao   +7 more
semanticscholar   +1 more source

Topologically inverse microstructure in single-crystal superalloys: microstructural stability and properties at ultrahigh temperature

open access: yesMaterials Research Letters, 2021
Topological phase inversion, in which γ'-precipitate becomes topological matrix phase, is a typical ‘detrimental’ microstructural degradation in Ni-based single-crystal superalloys.
Y. Ru   +7 more
semanticscholar   +1 more source

Research progress in effect of Ru on solidification characteristics, precipitation of topologically close-packed phases and creep property of nickel-based single crystal superalloy

open access: yesCailiao gongcheng, 2022
Nickel-based single crystal superalloys are widely used for hot components of advanced turbine engines due to their excellent mechanical properties at elevated temperature.
CAO Kaili   +7 more
doaj   +1 more source

Current situation of research on test methods for elastic modulus and Poisson’s ratio of single crystal superalloys

open access: yesJournal of Aeronautical Materials, 2019
In view of the anisotropic characteristics of elastic constants of single crystal superalloys and other materials, this paper summarizes two main existing testing methods for measuring elastic moduli and Poisson’s ratio of single crystal superalloys ...
ZHAO Pengtao, YU Huichen, HE Yuhuai
doaj   +1 more source

Mechanisms of High Temperature Degradation of Thermal Barrier Coatings. [PDF]

open access: yes, 2009
Thermal barrier coatings (TBCs) are crucial for increasing the turbine inlet temperature (and hence efficiency) of gas turbine engines. The thesis describes PhD research aimed at improving understanding of the thermal cycling failure mechanisms of ...
Wu, Rudder T.C., Wu, Rudder T.C.
core   +1 more source

Molecular dynamics simulations of dynamics mechanical behavior and interfacial microstructure evolution of Ni-based single crystal superalloys under shock loading

open access: yesJournal of Materials Research and Technology, 2021
In this paper, molecular dynamics simulations are performed to study the dynamic mechanical response and microstructural evolution of Ni-based single crystal superalloys under different shock velocities. The results show that when the shock velocity (Up ≤
Bin Chen, Wen-Ping Wu
doaj   +1 more source

Effect of rhenium on low cycle fatigue behaviors of Ni-based single crystal superalloys: a molecular dynamics simulation

open access: yesJournal of Materials Research and Technology, 2022
Molecular dynamics simulations are carried out to investigate the effects of rhenium (Re) on low cycle fatigue behaviors and deformation mechanisms of Ni-based single crystal superalloys.
Wen-Ping Wu   +4 more
doaj   +1 more source