Results 1 to 10 of about 10,456 (224)
Additive manufacturing is an advanced forming method to fabricate complex components, while cracks appear in the deposited nickel-based single crystal superalloy samples undesirably.
Zhipeng Zhou +5 more
doaj +3 more sources
Numerical Simulation on Pulsed Laser Ablation of the Single-Crystal Superalloy Considering Material Moving Front and Effect of Comprehensive Heat Dissipation [PDF]
In the present research, an iterative numerical model is proposed to investigate the nanosecond pulsed laser ablation (PLA) mechanism of the DD6 single-crystal superalloy.
Bin Wang +6 more
doaj +2 more sources
Application research progress of hot isostatic pressing technology in nickel-based single crystal superalloy [PDF]
Since the introduction of hot isostatic pressing (HIP) technology, it has been widely used in powder metallurgy forming and improving the densification of castings. With the increasing demand for the performance of nickel-based single crystal superalloy,
Wang Jun, Jiang Zhaojun
doaj +1 more source
Normalized Parameter Creep Model of DD6 Nickel-Based Single Crystal Superalloy
For nickel-based single crystal superalloy DD6 (AECC Beijing Institute of Aeronautical Materials, Beijing, China) material, a method for predicting creep rupture time was proposed based on a newly defined equivalent stress method.
Dasheng Wei +4 more
doaj +1 more source
The grain selector method is a prevailing technique in the manufacturing process of Ni-based single crystal superalloy, however, it cannot control the orientation of single crystal within an appropriate scope.
Binqiang Wang +4 more
doaj +1 more source
Through creep measurement and microstructure observation, the microstructure evolution and deformation mechanism of a [111]-oriented nickel-based single-crystal superalloy at 980 °C/186 MPa were studied.
Guangyan Wang +5 more
doaj +1 more source
Probing single crystal orientation by X-ray diffraction for nickel-based superalloys
The deviation angles of Ni-based single crystal superalloys are investigated by two techniques of rotating orientation X-ray diffraction (RO-XRD) and back-reflection Laue X-ray diffraction (BRL-XRD).
Yumin Wang +3 more
doaj +1 more source
In this study, the third-generation rhenium containing single crystal superalloy was brazed by mixed powder filler, in which the mixed powder filler was consisted of nickel-based powder filler and the superalloy powder with the same composition of the ...
LI Kexin +8 more
doaj +1 more source
On Crystal Mosaicity in Single Crystal Ni-Based Superalloys [PDF]
In the present work, we investigate the evolution of mosaicity during seeded Bridgman processing of technical Ni-based single crystal superalloys (SXs). For this purpose, we combine solidification experiments performed at different withdrawal rates between 45 and 720 mm/h with advanced optical microscopy and quantitative image analysis.
Philipp Hallensleben +6 more
openaire +3 more sources
At the conditions of 760℃/800 MPa, 980℃/250 MPa and 1100℃/137 MPa, the transv-erse stress rupture properties of a nickel-based third generation single crystal superalloy were investigated.
YANG Wan-peng +5 more
doaj +1 more source