Results 11 to 20 of about 10,456 (224)
Vibration Fatigue Properties and Fracture Mechanism of DD6 Single Crystal Superalloy
Room Temperature vibration fatigue S-N curves of single crystal superalloy DD6 with[001] orientation was investigated and room temperature vibration fatigue limit was obtained. The fracture mechanism was studied by OM, SEM and EBSD. The results show that
LIU Li-yu +3 more
doaj +1 more source
Joining single crystal superalloy with polycrystalline superalloy has important applications in the aerospace industry. Here, the IC10 single crystal superalloy to GH536 polycrystalline superalloy was diffusion brazed using a BNi-2 filler alloy.
Tong Wu +9 more
doaj +1 more source
The effect of thermal cycling on the high-temperature creep behaviour of a single crystal nickel-based superalloy [PDF]
Isothermal and thermal cycling creep behaviours of a single crystal nickel-based superalloy have been studied by means of tensile tests at 1150 °C and 80 MPa.
Andrieu, Eric +3 more
core +2 more sources
Mechanisms of High Temperature Degradation of Thermal Barrier Coatings. [PDF]
Thermal barrier coatings (TBCs) are crucial for increasing the turbine inlet temperature (and hence efficiency) of gas turbine engines. The thesis describes PhD research aimed at improving understanding of the thermal cycling failure mechanisms of ...
Wu, Rudder T.C., Wu, Rudder T.C.
core +1 more source
Deformation compatibility in a single crystalline Ni superalloy [PDF]
Deformation in materials is often complex and requires rigorous understanding to predict engineering component lifetime. Experimental understanding of deformation requires utilization of advanced characterization techniques, such as high spatial ...
Britton, T, Dunne, F, Jiang, J, Zhang, T
core +2 more sources
Thermomechanical fatigue in single crystal superalloys [PDF]
Thermomechanical fatigue (TMF) is a mechanism of deformation which is growing in importance due to the efficiency of modern cooling systems and the manner in which turbines and associated turbomachinery are now being operated. Unfortunately, at the present time, relatively little research has been carried out particularly on TMF of single crystal (SX ...
Moverare Johan J., Reed Roger C.
openaire +2 more sources
Fretting fatigue behavior of Ni-base superalloys used in gas turbine blades and disk assemblies have been investigated under ambient and high temperature conditions. A major emphasis was placed on the influence of experimentally measured tangential force
Balavenkatesh RENGARAJ +2 more
doaj +1 more source
Oxygen changes crack modes of Ni-based single crystal superalloy
Oxygen-affected cracking commonly presents on thin Ni-based single crystal superalloy components serving in high temperature and oxidizing environments.
Xueqiao Li +15 more
doaj +1 more source
Recrystallization of single crystal superalloy CMSX-4 casting
Single crystal plate castings of superalloy CMSX-4 were prepared, providing simplified geometries of turbine blades featured with five stage platforms. The recrystallization behavior in the plate castings was investigated after solution heat treatments ...
XU Fuze +5 more
doaj +1 more source
Static and dynamic aspects of coupling between creep behavior and oxidation on MC2 single crystal superalloy at 1150 °C [PDF]
Creep tests were performed on thin wall specimens made of MC2 single crystal superalloy at 1150 °C and under controlled atmosphere. The results highlight the deleterious oxidation effect on creep properties.
Andrieu, Eric +3 more