Research on vacuum-electromagnetic casting of IN100 superalloy ingots
In order to improve the inner quality of superalloy master alloy ingots, the new technology of superalloy vacuum-electromagnetic casting, i.e. applying electromagnetic stirring (EMS) to the solidification process of superalloy vacuum casting was ...
Wenzhong Jin, Tingju Li and Guomao Yin
doaj +1 more source
High-Throughput Data Generation and Transfer Learning Enabled Microstructure-Property Integrated Design of Nickel-Based Powder Metallurgy Superalloy. [PDF]
An integrated transfer learning framework integrates CALPHAD simulations, diffusion‐multiple experiments, and literature data to predict long‐term microstructural stability and short‐term mechanical properties of Ni‐based powder metallurgy superalloys. Based on these model predictions, a high‐performance, low‐density alloy, USTB‐PM750, is designed from
Li Z +8 more
europepmc +2 more sources
An investigation into cracking in nickel-base superalloy repair welds [PDF]
The nickel-base superalloy Rene 80 is considered very susceptible to liquation and strain-age cracking. Material in the solutionised condition is welded using the Cold Metal Transfer, or CMT process (with ductile filler alloy) and autogenously using a
Colegrove, Paul A. +7 more
core +1 more source
Nickel-Base Superalloy Precipitation - Superalloy Lecture 11
This set of lectures is on "Nickel-Base Superalloy Precipitation" for the Superalloys & High Performance Materials course part 11. This part of the course was taught by Dr Alec Davis at The University of Manchester in 2021.
Materials Engineering +1 more
core +1 more source
Influence of coating on the thermal resistance of a Ni-Based superalloy [PDF]
In this paper, the influence of M-CrAlY polycrystalline coating on the thermal fatigue behavior of a Nickel-base superalloy has been investigated. A special device using a rotating bending machine and two thermal sources has been used to perform thermo ...
Stephan, Nicolas +2 more
core +1 more source
Effects of microstructure on room temperature fatigue crack initiation and short crack propagation in Udimet 720Li Ni-base superalloy [PDF]
An assessment of the effects of microstructure on room temperature fatigue crack initiation and short crack propagation in a Ni-base superalloy is presented.
Pang, H.T., Reed, P.A.S.
core +1 more source
Liquation and post-weld heat treatment cracking in Rene 80 laser repair welds [PDF]
An extensive experimental study on a nickel-based superalloy, Rene 80 using autogenous laser welding has been undertaken to determine the effect of the process parameters and weld bead geometry on cracking in the as-welded and post- weld heat treated ...
Colegrove, Paul A. +7 more
core +1 more source
Investigation of delamination mechanisms during a laser drilling on a cobalt-base superalloy [PDF]
Temperatures in the high pressure chamber of aircraft engines are continuously increasing to improve the engine efficiency. As a result, constitutive materials such as cobalt and nickel-base superalloys need to be thermally protected.
SCHNEIDER, Matthieu +4 more
core +1 more source
Effect of Pre-Post TIG Welding Heat Treatment on Cast NI Superalloy
The effect of a pre (before) and post (after) heating welding treatment on the microstructure and mechanical properties of the scrap blades made of cast INC738LC superalloy is the main goal of the present investigation. The filler used in TIG welding was
C. Saib +4 more
doaj +1 more source
Studying the effect of Ruthenium on High Temperature Mechanical Properties of Nickel Based Superalloys and Determining the Universal Behavior of Ruthenium at Atomic Scale with respect to alloying elements, Stress and Temperature [PDF]
Any property of a material is a function of its microstructure and microstructure is a function of material composition. So, to maximize the desired properties of a material, one has to understand the evolution of microstructure which in turn is nothing ...
Sriswaroop Dasari
doaj +2 more sources