Results 21 to 30 of about 26,613 (245)

Study of the Creep Behavior of Nickel-Based Single Crystal Superalloy Micro Specimens with Dimensional Effects

open access: yesCrystals, 2022
Nickel-based single-crystal superalloys are widely used in aeroengine hot-end components, owing to their unique crystal structure and outstanding high-temperature mechanical properties.
Wangjiao Xiong   +7 more
doaj   +1 more source

Causes analysis on cracks in nickel-based single crystal superalloy fabricated by laser powder deposition additive manufacturing

open access: yesMaterials & Design, 2018
Additive manufacturing is an advanced forming method to fabricate complex components, while cracks appear in the deposited nickel-based single crystal superalloy samples undesirably.
Zhipeng Zhou   +5 more
doaj   +1 more source

Investigation on Optimal Ta/Cr Ratio of a Single Crystal Ni-Base Superalloy in View of the Isothermal Oxidation Behavior

open access: yesCrystals, 2021
The relative content of strengthening element tantalum (Ta) and oxidation-resistant element chromium (Cr) is an essential value for superalloys to obtain an excellent combination of oxidation resistance and mechanical properties.
Jianxiu Chang   +7 more
doaj   +1 more source

The effect of precious metals in the NiAl coating on the oxidation resistance of the Inconel 713 superalloy [PDF]

open access: yesJournal of Mining and Metallurgy. Section B: Metallurgy, 2022
The rhodium incorporated aluminide coating was produced by the rhodium electroplating (0.5 μm thick layer) followed by the chemical vapor deposition process on the Inconel 713 superalloy. This coating is composed of the β-NiAl phase.
Zagula-Yavorska M., Romanowska J.
doaj   +1 more source

Temperature evolution and grain defect formation during single crystal solidification of a blade cluster [PDF]

open access: yesChina Foundry, 2017
In order to investigate the asymmetry of thermal conditions during directional solidification, the temperature evolution and correspondingly developed undercooling in a simplified single crystal blade cluster were numerically simulated.
De-xin Ma, Fu Wang, Qiang Wu
doaj   +1 more source

Influence of Surface Roughness on the High Temperature /High Strain Low Cycle Fatigue Behavior of Nickel-Based Superalloy Rene®80 [PDF]

open access: yesArchives of Metallurgy and Materials, 2023
Since fatigue cracks nucleate and initiate generally at the surface of the rotary components such as blades and discs, the surface condition is the most important factor affecting the fatigue life.
Mohammad Mehdi Barjesteh
doaj   +1 more source

Numerical Simulation of Transport Phenomena in Directional Solidification Castings with Changeable Cross-Section and Solidification Interface Control

open access: yesMetals, 2022
The roles of traveling magnetic fields (TMFs) within the transport phenomena during the directional solidification of nickel-based superalloys were simulated.
Yanbin Zhang   +6 more
doaj   +1 more source

Hot extrusion characteristics and technique optimization for superalloy 617B tube

open access: yes工程科学学报, 2019
Nickel-base superalloy 617B is one of the most promising candidates for superheater and reheater pipes of advanced ultra-supercritical (AUSC) power plants.Hot extrusion is a key process during the manufacturing of superalloy 617B pipes.However, the high ...
JIANG He, DONG Jian-xin, ZHANG Mai-cang
doaj   +1 more source

Effects of Multi-electromagnetic Field on the Solidification Structure of IN100 Superalloy Castings

open access: yesHigh Temperature Materials and Processes, 2015
IN100 superalloy castings were vacuum cast with the application of multi-electromagnetic field. The effect of multiple-electromagnetic field on the solidification structure of IN100 superalloy castings has been studied.
Jin Wenzhong   +3 more
doaj   +1 more source

Friction Stir Welding of Ti-6Al-4V Using a Liquid-Cooled Nickel Superalloy Tool

open access: yes, 2022
Friction stir welding (FSW) of titanium alloy was carried out using liquid cooling of the FSW tool made of heat-resistant nickel superalloy. Cooling of the nickel superalloy tool was performed by means of circulating water inside the tool. The FSW joints
Andrey Chumaevskiy   +7 more
core   +1 more source