Results 81 to 90 of about 64,035 (272)

Investigation of Creep Properties of Ti‐43Al‐5V‐4Nb Alloy Considering Oxidation Effects Using Miniature Specimens

open access: yesFatigue &Fracture of Engineering Materials &Structures, EarlyView.
ABSTRACT In the present study, creep tests of a TiAl alloy were conducted using miniature specimens (d = 2 mm) under various conditions to investigate their creep properties at 760°C. The test results indicate that creep rupture time obtained using miniature specimens at identical applied stress levels increase with the order of test condition Ar gas ...
Lei He, Takamoto Itoh, Noritake Hiyoshi
wiley   +1 more source

High Cycle Fatigue Properties of PM‐HIPed High‐Nitrogen Tool Steel: Effect of Surface Condition

open access: yesFatigue &Fracture of Engineering Materials &Structures, EarlyView.
ABSTRACT This study explores the impact of surface condition on high‐cycle fatigue performance of a high‐nitrogen martensitic tool steel manufactured through powder metallurgy and hot isostatic pressing. In near‐net manufacturing applications, acid‐leaching pickling treatment and/or machining is used as a post‐treatment to remove the powder container ...
Faezeh Javadzadeh Kalahroudi   +3 more
wiley   +1 more source

MXene‐Based Materials Contribute Better Alkali Metal–Chalcogen Batteries: Progress, Challenges, and Perspectives

open access: yesRare Metals, Volume 45, Issue 4, April 2026.
ABSTRACT Alkali metal–chalcogen batteries (AMCBs) are one of the most promising next‐generation energy storage systems because of their high energy density and reasonably low cost. However, the practical application of AMCBs is severely hindered by the volume expansion of the chalcogen cathode, the shuttle effect of polychalcogenides, and unstable ...
Yong Liu   +11 more
wiley   +1 more source

Navigating the Ethereal Tightrope: The Nanogenerator Manipulates Neurons for Immune Equilibrium

open access: yesAdvanced Science, Volume 13, Issue 14, 9 March 2026.
This review explores how nanogenerators modulate neuroimmune responses, offering innovative strategies for treating neurological disorders. By interfacing with neural pathways, they enable precise control of immune activity, especially via vagus nerve stimulation.
Jia Du   +5 more
wiley   +1 more source

Data from: A 3D Analysis of Dendritic Solidification and Mosaicity in Ni-Based Single Crystal Superalloys

open access: green, 2021
F. Scholz   +5 more
openalex   +1 more source

Estimation of the engineering elastic constants of a directionally solidified superalloy for finite element structural analysis [PDF]

open access: yes
The temperature-dependent engineering elastic constants of a directionally solidified nickel-base superalloy were estimated from the single-crystal elastic constants of nickel and MAR-MOO2 superalloy by using Wells' method.
Abdul-Aziz, Ali, Kalluri, Sreeramesh
core   +1 more source

Deformable Eutectic Alloy With Near‐Theoretical Yield Strength via Hierarchical Nanoscale Multiphases and Sessile Defects

open access: yesAdvanced Science, Volume 13, Issue 14, 9 March 2026.
A CoCrFeNiTa0.4 eutectic high‐entropy alloy achieves a near‐theoretical yield strength of 2.6 GPa with 13.6% plasticity. This breakthrough stems from a hierarchical nanostructure (FCC‐Laves lamellae with L12/D022 precipitates), which alleviates the inter‐phase modulus/hardness mismatch through synergistic strengthening and toughening, guiding the ...
Yusha Luo   +10 more
wiley   +1 more source

SciLitMiner: An Intelligent System for Scientific Literature Mining and Knowledge Discovery

open access: yesAdvanced Intelligent Systems, Volume 8, Issue 3, March 2026.
SciLitMiner is an intelligent system that federately ingests scientific literature, filters it using advanced information retrieval methods, and applies retrieval‐augmented generation tailored to scientific domains. Demonstrated on creep deformation in γ‐TiAl alloys, SciLitMiner provides a controlled workflow for systematic knowledge discovery and ...
Vipul Gupta   +3 more
wiley   +1 more source

Effect of thermal cycling frequency on the durability of Yb-Gd-Y-based thermal barrier coatings [PDF]

open access: yes, 2019
The effects of thermal cycling frequency and buffer layer on the crack generation and thermal fatigue behaviors of Yb–Gd–Y-stabilized zirconia (YGYZ)-based thermal barrier coatings (TBCs) were investigated through thermally graded mechanical fatigue ...
Choi, Baig-Gyu   +5 more
core   +1 more source

Microstructural and Nanomechanical Characterization of CrCoAlHf/YSZ Multilayer Coatings Deposited by DC/RF Magnetron Sputtering

open access: yesInternational Journal of Ceramic Engineering &Science, Volume 8, Issue 2, March 2026.
A dense Cr/CoAlHf/YSZ multilayer coating was successfully deposited on Inconel 718 by DC/RF magnetron sputtering at 300°C. The coating exhibits nanocrystalline stability, strong interlayer adhesion, enhanced hardness, and excellent chemical integrity, making it suitable for advanced high‐temperature aerospace applications.
Syed Faizan Altaf   +2 more
wiley   +1 more source