Results 101 to 110 of about 17,583 (228)

The hot corrosion of nickel-base disc alloys [PDF]

open access: yes, 2011
The efficiency of a jet’s engines has a direct affect on its economic and environmental impact through the quantity of aviation fuel consumed and CO2 emitted.
Potter, Andrew
core   +1 more source

Directional solidification of superalloys [PDF]

open access: yes, 1990
This invention relates to the directional solidification of superalloys, in particular nickel-based superalloys, by imposition of a predetermined temperature profile in the solidification front and, depending on the desired results, a predetermined rate ...
Alter, Wendy Sue   +2 more
core  

Laser cladding for epitaxial nickel base superalloys turbine blades [PDF]

open access: yes, 2014
Dissertação (mestrado) - Universidade Federal de Santa Catarina, Centro Tecnológico, Programa de Pós-Graduação em Engenharia Mecânica, Florianópolis, 2014.A prosperidade e larga utilização da aviação como meio de transporte civil, nacional e ...
Schweitzer, Luiz Guilherme de Souza
core  

Research on a Stability Control Strategy for Braking Failure in Distributed-Drive Electric Vehicles

open access: yesApplied Sciences
Distributed-drive electric vehicles (DDEVs) improve braking stability through independent four-wheel braking torque control, yet their complex multi-brake systems are prone to braking faults that cause loss of longitudinal and yaw stability.
Sheng Yong   +4 more
doaj   +1 more source

Nasa developments in cobalt-base superalloys [PDF]

open access: yes, 1964
Chemical, mechanical and physical properties of cobalt-refractory-metal superalloys for high temperature aerospace ...
Freche, J. C.   +2 more
core  

Oxidation resistant claddings for superalloys [PDF]

open access: yes, 1971
Oxidation protection of superalloys by thin claddings of Ni-Cr-Al-Si and Fe-Cr-Al-Y alloys examined and compared with commercial aluminide ...
Gedwill, M. A., Grisaffe, S. J.
core  

Crystallographic Constitutive Models for Single Crystal Superalloys

open access: yes, 2011
Single crystal nickel base superalloys, such as Chinese material DD6 have been used in gas turbine blade in China more and more widely. In order to make better use of single crystal superalloys with many excellencies, constitutive models have been ...
Shi Hui Zhang, Qing Wu Wang, Mao Pang
core   +1 more source

Surface patterning for multi-scale strain analysis of in-situ SEM mechanical experiments

open access: yesJournal of Materials Research and Technology
Scanning electron microscopy (SEM) enables microstructure characterization at multi-scale, having potential to quantify strain distribution across multiple fields of view (FOVs) and exploring coordinated relationships among the deformations of multi ...
Bin Zhang   +4 more
doaj   +1 more source

Diffusion welding of nickel-based superalloys [PDF]

open access: yes, 2011
Ni based superalloys can be welded by diffusion bonding. Temperature, diffusion coefficient, activation energy and Boltzmann constant influence the quality of diffusion bonding, so obtaining the best condition for welding is considered.
Rezaei, Hossein
core   +2 more sources

Thermal management in grinding of superalloys – A critical review [PDF]

open access: yes
Purpose – This paper is supposed to provide a critical review of current research progress on thermal management in grinding of superalloys, and future directions and challenges.
Wenfeng Ding   +4 more
core   +1 more source