Results 41 to 50 of about 17,583 (228)

Non‐Additive Criteria Assessment in Sustainability Evaluation of High Entropy Alloys: A Toxicity‐Weighted Framework

open access: yesAdvanced Engineering Materials, EarlyView.
Sustainability assessment requires methodologies that appropriately distinguish between additive and non‐additive material properties. A toxicity‐weighted scoring system is developed and applied that accounts for the disproportionate influence of highly toxic constituents through nonlinear weighting functions, providing more realistic estimates than ...
Seth Mehalic   +2 more
wiley   +1 more source

Microstructural Evolution of a Re-Containing 10% Cr-3Co-3W Steel during Creep at Elevated Temperature

open access: yesMetals, 2023
Ten percent Cr steels are considered to be prospective materials for the production of pipes, tubes, and blades in coal-fired power plants, which are able to operate within ultra-supercritical steam parameters.
Alexandra Fedoseeva   +4 more
doaj   +1 more source

High‐Entropy Alloy Interlayers Toward Advanced Joining for High‐Performance Structural Applications: Current Progress and Emerging Challenges

open access: yesAdvanced Engineering Materials, EarlyView.
HEA interlayers offer a versatile route for joining high‐performance structural materials. Their compositional and structural design regulates interfacial reactions, suppresses brittle IMCs, and improves metallurgical bonding. Sandwich interlayers further integrate defect healing with precipitation strengthening, enabling improved strength–ductility ...
Lin Yuan   +4 more
wiley   +1 more source

Effect of Tungsten on Creep Behavior of 9%Cr–3%Co Martensitic Steels

open access: yesMetals, 2017
The effect of increasing tungsten content from 2 to 3 wt % on the creep rupture strength of a 3 wt % Co-modified P92-type steel was studied. Creep tests were carried out at a temperature of 650 °C under applied stresses ranging from 100 to 220 MPa with a
Alexandra Fedoseeva   +3 more
doaj   +1 more source

Cryogenic Deformation Behavior of TiAl and Insights Into Embrittlement After High‐Temperature Exposure Combined With Secondary Ion Mass Spectroscopy of Near Surface Chemistry

open access: yesAdvanced Engineering Materials, EarlyView.
Near‐surface deuterium enrichment profiles for different microstructural types of TiAl after exposure at 700 °C in a heavy water‐containing environment. The deuterium levels are significantly higher than expected from natural occurrence, indicating that the heavy water dissociated during the exposure treatment and entered the specimens.
Jonathan D. H. Paul   +5 more
wiley   +1 more source

Precipitation kinetic modeling of the new eta-phase Ni6AlNb in Ni-base superalloys

open access: yes, 2016
Eta phase stabilities were evaluated in consideration of new experimental data on the Ni-base superalloy, ATI718Plus. It has been found that the previously suggested miscibility between Ni3Ti (η-phase) and the Ni6NbAl compound (η*-phase) has ...
Povoden-Karadeniz, Erwin   +2 more
core   +1 more source

Unlocking High Ductility in a High-Strength Titanium Alloy via Cooling-Rate-Controlled Dual-Phase Connectivity

open access: yesMetals
The strength–ductility trade-off limits the wider application of high-strength titanium alloys in aerospace. Here, a new Ti-3.7Al-3V-3Fe-1.7Mo-0.5Cr alloy is designed based on d-electron alloy design theory and molybdenum equivalence, and the dual-phase ...
Keyi Li   +11 more
doaj   +1 more source

Mitigating Creep Anisotropy and Enhancing Performance in Additively Manufactured Ni‐Based Superalloys: A Review

open access: yesAdvanced Engineering Materials, EarlyView.
Additive manufacturing introduces pronounced microstructural and crystallographic anisotropy in Ni‐based superalloys, resulting in orientation‐dependent creep deformation and damage. This review identifies the key microstructural origins of creep anisotropy, examines their influence on dominant deformation mechanisms, and highlights processing ...
Chandan Kumar   +3 more
wiley   +1 more source

The Evolution of Abnormal Grains during the Heating Stage of a Post-Weld Solution Treatment in a Friction-Stir-Welded 2519 Aluminium Alloy

open access: yesMetals, 2023
This work presents an in-depth investigation of the early stages of abnormal grain growth (AGG) in a friction-stir-welded (FSWed) 2519-T820 aluminium alloy. Microstructural evolutions, which occurred during the heating stage of a solution heat treatment (
Ivan S. Zuiko   +4 more
doaj   +1 more source

Sustainable Materials Design With Multi‐Modal Artificial Intelligence

open access: yesAdvanced Science, EarlyView.
Critical mineral scarcity, high embodied carbon, and persistent pollution from materials processing intensify the need for sustainable materials design. This review frames the problem as multi‐objective optimization under heterogeneous, high‐dimensional evidence and highlights multi‐modal AI as an enabling pathway.
Tianyi Xu   +8 more
wiley   +1 more source