Results 131 to 140 of about 8,287,589 (343)
THERMAL-DEGRADATION OF BLENDS OF PVC WITH POLYDIMETHYLSILOXANE
The thermal degradation of blends of PVC with polydimethylsiloxane (PDMS) has been studied by thermogravimetry (TG) over the whole composition range and by thermal volatilisation analysis (TVA) for 1:1 by weight blends. From the TG data, curves have been
BASAN, S, MCNEILL, IC
core +1 more source
CT‐based finite element simulations combined with in situ X‐ray computed tomography are used to analyze insert pull‐out in nickel‐coated polymer foams. Despite variations in material parameters, deformation consistently concentrates within a narrow annular region around the insert.
Yannik Bautz +4 more
wiley +1 more source
The thermal behaviour and degradation mechanism of fully aromatic polyester, poly(oxy-1,4-phenyleneoxy-fumaroyl-bis-4-oxybenzoate), were studied by pyrolysis-gas chromatography and pyrolysis-gas chromatography/mass spectrometry at 500-700°C, and by ...
Zuev VV, Bertini F
core
Characteristics of kenaf fibre/epoxy composites subjected to thermal degradation
Kenaf fibres are receiving much attention in the natural fibre composite industry due to its potential as polymer reinforcements. However, like all natural fibres, kenaf fibres have lower thermal resistance as compared to synthetic fibres.
Yousif, B. F., Azwa, Z. N.
core +1 more source
Fabrication Routes for Ionic Conducting Fiber Strain Sensors
Ionic conducting fiber strain sensors (ICFSs) offer compliant, textile‐integrable sensing. Thus far, the commercialization of ICFSs has been constrained by fiber fabrication routes. This review provides a fabrication‐centric analysis of ICFSs correlating processing strategies with material properties and scalability.
Leo John Kershaw +3 more
wiley +1 more source
Gallium microalloying redirects interfacial reactions in low‐temperature Bi–Sn solders from Cu–Sn toward Cu–Ga intermetallic formation. The resulting Cu–Ga layer suppresses intermetallic growth during thermal aging, alters fracture pathways, and improves interfacial stability.
Iva Králová +6 more
wiley +1 more source
Feasibility and Limitations of the Advanced Replica Process for Bioactive Glasses
Periodic 3D‐printed Kelvin‐cell templates enable a controlled advanced replica process for fabricating highly porous glass lattices. Across P45K9, 45S5, and 13–93, material‐dependent differences in coating, burnout, and shrinkage lead to distinct strut morphologies, while comparable final porosities of 83%–88% are retained.
Swantje Funk +4 more
wiley +1 more source
The thermal behaviour and degradation of an alkylene-aromatic liquid crystalline polyester, poly(decamethylene-fumaroyl-bis-4-oxybenzoate), were studied by thermogravimetric analysis under dynamic conditions and by pyrolysis-gas chromatography and ...
Zuev VV, Bertini F
core +1 more source
HEA interlayers offer a versatile route for joining high‐performance structural materials. Their compositional and structural design regulates interfacial reactions, suppresses brittle IMCs, and improves metallurgical bonding. Sandwich interlayers further integrate defect healing with precipitation strengthening, enabling improved strength–ductility ...
Lin Yuan +4 more
wiley +1 more source
Effect of montmorillonite treatment on the thermal stability of poly(vinyl chloride) nanocomposites
The aim of this research was to study the effect of different intercalants on the thermal degradation/dehydrochlorination of poly(vinyl chloride) (PVC). PVC nanocomposites were prepared containing 2 phr of montmorillonite clay.
Jacobsen, Harald +8 more
core +1 more source