Results 21 to 30 of about 2,611,574 (280)
The load partitioning between the magnesium and titanium phases in an extruded Mg-15%Ti (vol.%) composite from room temperature up to 300 °C using synchrotron radiation diffraction during in-situ compression tests.
G. Garces +5 more
doaj +1 more source
Effect of Boron and Tungsten Carbides on the Properties of TiC-Reinforced Tool Steel Matrix Composite Produced by Powder Metallurgy [PDF]
The influence of boron carbide and tungsten carbide on the apparent porosity, density, coercive force, hardness and microstructure of metal matrix composite of the Ferro-TiC type, is presented in this paper.
Ljerka Slokar Benić +2 more
doaj +1 more source
The influence of acrylate triblock copolymer embedded in matrix on composite structures’ responses to low-velocity impacts [PDF]
In passive safety structures the use of composite materials has increased significantly recently due to their low specific mass and high energy absorption capacities.
Frédéric Leonardi +7 more
core +1 more source
This study examined the effects of different carbon nanomaterials on the mechanical and tribological properties of titanium matrix composites. Carbon nanotubes (CNTs), graphene nanoplates (GNPs) and graphene oxide nanoplates (GOs) reinforced Ti–6Al–2Sn ...
Jiashi Yu +7 more
doaj +1 more source
Microstructure Characterization of Composite from ZrO2 – Ti System
In this work the microstructure analysis of composite from ZrO2 – Ti system were presented. For the preparation of the composite samples nanometric ZrO2 powder stabilized by 3 mol% of Y2O3 and micrometric titanium powder were used. The composites with 10
Łada P. +3 more
doaj +1 more source
Wear Behavior of Self-mated Ti-Si-C Composites and Ti-Si-N Composites Slid Without Lubricant
To develop lightweight wear-resistant titanium matrix composites, the wear behaviors of three kinds of composites produced from SiC and titanium (Ti-Si-C composite) and three kinds of composites produced from Si3N4, TiN and titanium (Ti-Si-N composite ...
Yuko Hibi, Takashi Murakami
doaj +1 more source
Pure Ti and Ti-6Al-4V alloy show high specific strength, excellent fatigue strength and good corrosion resistance; however, their poor wear resistance limits potentially wider application.
Hiroshi IZUI +2 more
doaj +1 more source
Laser surface modification of Ti alloys [PDF]
The laser surface engineering of titanium alloys has been developed over the past 30 years to produce a modified layer up to 1mm depth, thicker than alternative techniques.
Baker, T.N.
core +3 more sources
In the present work, magnesium matrix composite reinforced with titanium dioxide (TiO _2 ) nanoparticulates was synthesized using powder metallurgy (solid-state processing) technique followed by hybrid microwave heat treatment and hot extrusion ...
P C Elumalai, R Ganesh
doaj +1 more source
Titanium carbide coating on graphene nanoplatelets
Titanium carbide was formed on graphene nanoplatelets (GNPs) using potassium hexa-fluorotitanate (K2TiF6) salt in the presence of pure aluminium. K2TiF6 - GNPs mixture with titanium to carbon ratio of 5:1 was heated at a high temperature of 900 °C for 1 ...
Mahmood Khan +7 more
doaj +1 more source