Results 1 to 10 of about 174,552 (292)
The ferrovanadium slag sample was fused with sodium carbonate-boric acid at high temperature, then acidified with hydrochloric. Vanadium 310.230 nm, iron 259.940 nm, manganese 257.610 nm and phosphorus 213.618 nm were selected as the analytical lines ...
Qiongxian Liu +4 more
doaj +1 more source
Research Progress on Recovery of Scandium from Vanadium Titano- Magnetite in Panzhihua
Review on the occurrence state of scandium in Panzhihua vanadium titano- magnetite showed as Mg-Fe isomorphism, rich reserves and the recovery of considerable potential value.
Lufeng Wang, Yue'e Yan
doaj +1 more source
The research was based on the designed Ti–Al–Zr–Sn–Mo alloy for the application as structural material in marine area. TiC/TiB/Ti composite was fabricated via in situ synthesized, while Y2O3 nano-particles were added with the aim of refining grains and ...
Jiaping Han +6 more
doaj +1 more source
Vanadyum, çok farklı yükseltgenme basamağında bulunan, kolay yükseltgenmeyen, korozyona dayanıklı bir geçiş elementidir. Sert ve işlenebilir çelik, seramik, yarı iletken üretimi gibi birçok endüstriyel alanda vanadyum veya bileşikleri kullanılır. Sülfürik asit ve birçok organik bileşiğin üretimi gibi birçok alanda bileşikleri katalizör görevi görür ...
E Garribba, D Sanna
+6 more sources
In order to solve the problem of excessive degradation rate and insufficient biocompatibility of magnesium‐based bone implants, a polyphenol (EGCG) induced hydroxyapatite (HA) coating was prepared on the surface of AZ31 alloy.
Tao Chai +7 more
doaj +1 more source
The main useful metal mineral in the tin ore from Changning is cassiterite, followed by limonite, the main gangue mineral is quartz, and tin mainly exists in the form of cassiterite and acid soluble tin. The tin ore with tin grade of 0.166% and yield of −
Purong Wang, Guoyin Xu, Gang Su
doaj +1 more source
A New Method for Preparing Titanium Aluminium Alloy Powder
Due to TiAl alloys’ excellent properties, TiAl alloys have received widespread attention from researchers. However, the high energy consumption and lengthy process of traditional preparation methods have always limited the large-scale application of TiAl
Jialong Kang +4 more
doaj +1 more source
During continuous casting, argon blowing from tundish cover (ABTC) can greatly prevent the flow of the remaining air and decrease the reoxidation of molten steel in tundish.
Yang Li +6 more
doaj +1 more source
Corrosion behaviours of a LaB6/TiC/TiB/ti composite in neutral or acidic electrolytes
LaB6/TiC/TiB was incorporated into a Ti–Al–Zr–Sn alloy to achieve an efficient improvement in acid-resistance. The incorporation of LaB6/TiC/TiB deteriorated the performance of the passive layer, but impeded the penetration of the corrosive medium into ...
Jiaping Han +10 more
doaj +1 more source
The comprehensive utilization of metallurgical mineral solid waste is an important part of building a green and low-carbon circular economy system.
Jing Hou +5 more
doaj +1 more source