Results 71 to 80 of about 10,189,080 (188)

Evolution of friction and wear in rack-railway gear–rack pairs under heavy-load dry sliding conditions

open access: yesAIP Advances
Rack railways commonly operate under extreme conditions—steep gradients, heavy loads, and dry sliding—where wear of the gear–rack pair becomes a critical limitation to both safety and cost-effectiveness.
Haowei Yu   +3 more
doaj   +1 more source

Analytical model for predicting coverage in suspension waterjet shot peening and its influence on fatigue

open access: yesMaterials Research Express, 2023
Suspension waterjet peening is an emerging technology for surface modification. Coverage is a key factor affecting the integrity of a modified material surface, however such an experimental method that can be utilized for precise control has not yet been
Yongtao Ma   +6 more
doaj   +1 more source

Tailoring the Hardening Behavior of 18CrNiMo7-6 via Cu Alloying

open access: yes, 2016
In order to improve the rolling contact fatigue (RCF) behavior of gear steels, a concept to increase their damage tolerance is developed alternatively to the conventional approach of improving the degree of steel cleanliness. For that purpose, Cu is used
Bleck, Wolfgang   +20 more
core   +1 more source

Production Practice of 18CrNiMo7-6 Electroslag Process for High-speed Rail Gear Steel

open access: yesTeshugang, 2023
In order to achieve the goal of high cleanliness of high-speed gear steel,especially the size of single-Particle D spherical inclusions ≤10 μm, electroslag process was developed to produce high-speed rail gear steel 18CrNiMo7-6 (/%:0.15-0.21C, ≤0.40Si,0 ...
Wang Zhixiang, Nan hai, Zhang Jinwen
doaj  

sj-tif-6-pie-10.1177_09544089221080822 - Supplemental material for Experimental investigation on the effect of barrel finishing processes on surface integrity of 18CrNiMo7-6 carburized rollers

open access: yes, 2022
Supplemental material, sj-tif-6-pie-10.1177_09544089221080822 for Experimental investigation on the effect of barrel finishing processes on surface integrity of 18CrNiMo7-6 carburized rollers by Xiuhua Zhang, Huaiju Liu, Shaojie Wu, Gaomeng Li and ...
Xiuhua Zhang (486216)   +4 more
core   +1 more source

Research on the Influence of the Isothermal Normalizing Cooling Rate on the Mechanically Polished Surface Roughness of Wind Power Gear Blanks

open access: yesMetals
This study takes 18CrNiMo7-6 wind power gear steel as the object. Following the first holding stage of isothermal normalizing, the 18CrNiMo7-6 wind power gear blanks were cooled to the isothermal temperature via air cooling (AC) and forced-air cooling ...
Yuhao Wang   +5 more
doaj   +1 more source

Residual stresses in 18CrNiMo7-6 linear friction welded high strength steel chains

open access: yesThe International Journal of Advanced Manufacturing Technology, 2018
Linear friction welding is a solid-state process that comprises rapid heating and cooling of the welded parts. Residual stresses (RS) as in every other welding process cannot be avoided. The presence of RS compromises the in-service performance and reliability.
Garcia Nunes, Dinis   +5 more
openaire   +4 more sources

Quality of semi-finished steel product 18CrNiMo7-6 of carburized gears for wind energetics

open access: yes, 2012
Teoretická část diplomové práce se zabývá větrnou energetikou, druhy převodovek, materiály používanými pro ozubená kola, cementováním a nitrocementováním a napětími a deformacemi. Experimentální část je zaměřena na posouzení vlastností polotovarů z oceli
Hrdlička, Václav
core  

Evolution of Inclusions in Gear Steel 18CrNiMo7-6 during 70 t EAF-LF-RH Smelting Process

open access: yesTeshugang, 2022
The evolution of inclusions in gear steel 18CrNiMo7-6 produced by 70 t EAF + LF + RH process is systematically analyzed and studied by means of whole process sampling and ASPEX test.
胡梦頔
doaj  

Effect of Mould and Hot Top Design on Yield of 6 t Octagonal Ingot of Special Steels

open access: yesTeshugang, 2014
Based on the original 5 t (real 5. 15 t) octagonal ingot mould, with increasing the height of mould from original 1505 mm to 1840 mm, decreasing the taper in the mold walls from 4. 56% to 3.
沙卫星   +5 more
doaj  