Characteristics of tempering response of austempered ductile iron
Austempered ductile iron (ADI) is produced by an isothermal heat treatment. Tempering is an effective method to increase the toughness and decrease the hardness of ADI.
Bingxu Wang +4 more
doaj +2 more sources
Effect of the Annealing Temperature on the Microstructure and Properties of Ausferritic Nodular Cast Iron [PDF]
The paper presents the microstructure and selected properties of ausferritic nodular cast iron annealed at the temperature 520 and 550°C. This choice was dictated by the temperatures used in the practice of nitriding.
Gumienny G., Klimek L., Kurowska B.
doaj +2 more sources
Phase Transition Kinetics in Austempered Ductile Iron (ADI) with Regard to Mo Content. [PDF]
The phase transformation to ausferrite during austempered ductile iron (ADI) heat treatment can be significantly influenced by the alloying element Mo. Utilizing neutron diffraction, the phase transformation from austenite to ausferrite was monitored in ...
Landesberger M +6 more
europepmc +3 more sources
Fatigue of austempered ductile cast iron
A low alloy austempered ductile iron (ADI), with compn. 3.6C, 2.5Si, 0.6Mn, 0.15Mo, 0.3Cu (all wt%), was heat treated to investigate the effect of microstructure on the fatigue endurance.
Ivanishvili, G +4 more
core +7 more sources
Influece of the austempering temperature on the tensile strength of the austempered ductile iron (ADI) samples [PDF]
Austempered Ductile Iron (ADI) is a class of ductile iron subjected to a two-step heat treatment process – austenitization and austempering. The heat treatment gives to ADI a high value of tensile strength and an especially good strength-to-weight ratio.
S. Savićević +5 more
doaj +1 more source
Morphology and Crystallography of Ausferrite in Austempered Ductile Iron [PDF]
The microstructure of austempered ductile iron was investigated by electron backscatter diffraction technique. The results show that the orientation relationship between acicular bainitic ferrite and austenite is Greninger–Troiano relationship. A single austenite grain is divided into four packets and each packet contains six variants that share a {011}
Chengduo Wang +4 more
openaire +1 more source
The austempered ductile iron (ADI) grinding balls were austenitized at 900 °C for 2 h and then incomplete quenched in a sodium silicate solution for 100 s, after that austempered in an isothermal furnace at 230 °C for 1 h.
Hongyu Zhou, phD +8 more
doaj +1 more source
Evaluation of CADI Low Alloyed with Chromium for Camshafts Application
Different processing routes have been developed to increase the strength and hardness of camshafts for automotive applications. In this work, two carbidic austempered ductile irons (CADIs), alloyed with 0.2 and 0.4 wt% Cr, were evaluated to determine ...
Alejandro Cruz Ramírez +4 more
doaj +1 more source
EFFECT OF ANTIMONY ON THE WEAR RESISTANCE AND IMPACT TOUGHNESS OF CARBIDIC AUSTEMPERED DUCTILE IRON (CADI) [PDF]
This work investigated the effect of antimony on the impact toughness and wear resistance of carbidic austempered ductile iron (CADI). Six alloys with a carbon equivalent value of 4.44 (hyper-eutectic composition) were used to evaluate the produced CADI,
Barnabas Abel ADEIZA +2 more
doaj +1 more source
EVALUATION OF THERMAL STABILITY OF AUSFERRITE IN AUSTEMPERED DUCTILE IRON USING DIFFERENTIAL SCANNING CALORIMETRY [PDF]
Austempered Ductile Iron (ADI) is prone to changes in microstructure and mechanical properties when exposed to elevated service temperatures. Differential Scanning Calorimetry has been used to evaluate the stabilizing effects of copper, nickel ...
Warsinski, Karl, Karl Warsinski