Results 61 to 70 of about 557 (142)
Shot Peening of Austempered Ductile Iron [PDF]
Austempered ductile iron (ADI) is a type of heat-treated cast iron, which offers numerous positive advantages including: good combination of mechanical properties and damping characteristics, lower density than steel and the possibility of casting ...
Zammit, Ann
core +2 more sources
In-situ SEM observation on fracture behavior of austempered silicon alloyed steel [PDF]
Crack initiation, propagation and microfracture processes of austempered high silicon cast steel have been investigated by using an in-situ tensile stage installed inside a scanning electron microscope chamber.
Chen Xiang, Grahn Jonny, Vuorinen Esa
core
The paper presents the microstructure and selected properties of ausferritic nodular cast iron annealed at the temperature 520 and 550°C. This choice was dictated by the temperatures used in the practice of nitriding.
Gumienny G., Klimek L., Kurowska B.
doaj +1 more source
Austempering in Zamak bath : influence of austempering time and austenitizing temperature on ductile cast iron properties [PDF]
The combination of the austempered ductile iron mechanical properties strongly depend on the parameters used on the austempering cycle. On this study, the influence of austempering time and austenitizing temperature on the properties of a ductile iron ...
Amaral, Regis Fabiano do +5 more
core +1 more source
Effect of alloying elements on austempered ductile iron (ADI) properties and its process: Review [PDF]
Austempered ductile iron (ADI) parts have a unique combination of high strength and toughness with excellent design flexibility and low cost. These excellent properties are directly related to its microstructure called "ausferrite" that is the result of ...
Amir Sadighzadeh Benam
doaj
To meet the mechanical property requirements of gray cast iron for the shells of coal mine explosion-proof equipment and investigate the effect of austenitizing temperature on the microstructure and mechanical properties of gray cast iron, isothermal ...
Shian Zhu +6 more
doaj +1 more source
Microstructure, wear behavior and surface hardening of austempered ductile iron
Austempered ductile iron has been considered as a substitution to replace conventional steel castings, steel forgings and even aluminum in many applications.
Bingxu Wang +5 more
doaj +1 more source
Surface hardening and wear performance of ausferritic silicon steels
A special microstructure called ausferrite, consisting of ferrite laths surrounded by carbon supersaturated retained austenite can be created in steels containing more than about 1.5 % silicon. This structure, which is achieved by means of an austempering treatment, is fine-grained and free of carbides, presenting a good combination of ...
openaire +2 more sources
Effect of copper on the austempering behaviour of spheroidal graphite iron [PDF]
Two types of spheroidal graphite cast iron samples, one with Cu and other without Cu were austempered at four different temperatures. The austempering temperatures were 250 ˚C, 300 ˚C, 350˚C, 400˚C.
Khan, Ayaz, Tamuli, Kausik
core
Fabrication of forced air cool austempered ductile iron and exploring its corrosion behaviour in a simulated mine water [PDF]
: The production of austempered ductile iron (ADI) with uniform microstructure and properties is constrained by the austempering process vis-à-vis the quenching medium.
Aribo, Sunday +5 more
core +2 more sources