Study of Chemical Bath Deposited In2S3 Thin Films
Indum(III) sulfide (In2S3) thin films were grown by means of chemical bath deposition from acid solution. Calculation of ionic equilibrium with using of thermodynamic constants for systems defines boundary conditions of formation In2S3. Films were characterized by means of XRD, SEM, EDX and XPS methods.
Tulenin, S. S. +3 more
openaire +3 more sources
pH effect on structural, morphological and optical properties of ZnO thin films produced by chemical bath deposition method [PDF]
Zinc oxide (ZnO) thin films are widely used in the production of high value-added technological products such as photovoltic cells, sensors, flexible and wearable electronic materials, as they are abundant in nature, easy to process, low cost and can be ...
Fatih Gözükızıl, M.
core +1 more source
Synthesis of ZnO Nanoparticles using Blue and IR Laser-Assisted Chemical Bath for Water Degradation [PDF]
Water pollution is a pressing global issue that demands constant evaluation of water resource policy. It is responsible for causing deaths and diseases worldwide, with an approximate daily death toll of 14000 people.
Hind Abdulgafour +3 more
doaj +1 more source
Synthesis of PbS Nanostructures by Chemical Bath Deposition Method
Lead sulfide (PbS) powders were prepared by chemical bath deposition (CBD) method by varying the synthesis temperatures. The influence of the synthesis temperature and the different molar concentration of lead acetates on the structure, morphology and ...
L.F. Koao, F.B. Dejene, H.C. Swart
doaj +1 more source
Kinetics of chemical bath deposition of zinc sulfide ZnS
The paper is devoted to kinetic methods of chemical bath deposition of zinc sulfide ZnS from aqueous alkaline solutions containing ehylenediamine complex zinc salt Zn(En)n2+ and diamide of thiocarbonic acid N2H4CS.
A. A. Uritskaya +2 more
doaj +1 more source
CHEMICAL BATH DEPOSITION OF PbS THIN FILMS
In the current study, thin films of PbS were fabricated at 35 ᵒC bath temperature via chemical bath deposition (CBD) method. During the experiment, 0.1460 M NaOH and 0.0085 M Pb (NO3)2 were dissolved in 100 ml of deionized water and 0.510 M thiourea was inserted.
Metehan ÖNAL, Barış ALTIOKKA
openaire +4 more sources
Deposition of Composite Titania/Vanadia Thin Films by Chemical Bath Deposition [PDF]
Deposition of Composite Titania/Vanadia Thin Films by Chemical Bath ...
Rudolf C. Hoffmann (1625404) +4 more
core +1 more source
We deposited zinc-based films with various ammonia (ammonium hydroxide; NH4OH) and selenourea concentrations, at the bath temperature of 80 °C, on soda-lime glass substrates using the chemical bath deposition (CBD) process.
Chia-Hua Huang +3 more
doaj +1 more source
Deposition and characterization of Cu4SnS4 thin films by chemical bath deposition method
A low cost chemical bath deposition method has been used for the preparation of Cu4SnS4 thin films onto indium tin oxide glass substrate. The deposition parameters such as bath temperature (50 °C), deposition time (120 min), electrolyte concentration (0 ...
Anuar Kassim +4 more
doaj +1 more source
Preparation of ZnTe thin films using chemical bath deposition technique
Chemical bath deposition was used to prepare thin films of ZnTe. The density of compounds (0.5–2) ml in 50 ml of distilled water, the precipitation time (10–80 min), and the solution temperature during the precipitation process (15–85 °C) have been ...
Iman Ahmed Younus +2 more
doaj +1 more source