Results 51 to 60 of about 63,948 (294)
Study on strengthening during cold drawing of steel tubes
Study on strengthening during cold drawing was carried out on the samples taken from the steel tube before and after the cold drawing on drawing bench.
Brlić, Tin +4 more
core +1 more source
Effect of solution treatment on grain boundary structure of Inconel 617 alloy bar
The grain-boundary microstructure of Inconel 617 alloy hot-rolled rods during cold drawing and subsequent solution treatment is investigated using the electron backscattering diffraction (EBSD) technique. The results reveal that the microstructure of the
LU Jun +3 more
doaj +1 more source
Cold Drawing of Magnesium Alloy Tubes for Medical
Magnesium alloy is the lightest in practical metals, and it is used for housing small home appliance products and automobile parts. It is also expected to be a new material for stents, because of its possibility of systemic absorption. Fineness, thinness,
Kazunari Yoshida, Akinobu Koiwa
core +1 more source
This review highlights advances in lightweight, lead‐free polymer nanocomposites for diagnostic X‐ray shielding. By linking filler chemistry, dispersion, architecture, and photon interaction mechanisms, it establishes structure–performance relationships guiding material design.
Aklilu G. Messele +2 more
wiley +1 more source
In this work, a drawing processed was simulated to calculate forces and the resulting residual stresses in the material. The calculated residual stresses were compared with experimentally measured residual stresses by the Neutron Diffraction Method.
Tomaz Fantin de Souza +5 more
doaj
A Dislocation Perspective on Strength and Toughness in Ceramics
Dislocations in ceramics enjoy a long but yet under‐appreciated history. The three research waves for dislocations in ceramics highlight the topic evolution over the last 90 years. This review focuses on the impact of dislocation on strength and toughness in ceramics.
Xufei Fang
wiley +1 more source
The effect of cold-drawing on the creep behavior of a nickel-4.2 percent aluminum alloy
Creep tests were made at 700, 900, and 1200 °F (644, 755, and 921 °K) on a nickel-4.2 percent aluminum alloy (Duranickel) initially as cold-drawn and as cold-drawn and age-hardened.
Jenkins, William D.; Willard, William A.
core +1 more source
The nanostructure, size, and function of mRNA‐loaded lipid nanoparticles are evaluated before drying, within polymer microneedles, and after rehydration. The results reveal the polymer and LNP loadings required to recover nanostructure and preserve the delivery performance in dry‐state formulations.
Brendan P. Dyett +19 more
wiley +1 more source
Validation of results of two different reductions for precision seamless cold drawn tubes
This paper deals with the comparison of the seamless pulling process of precision seamless tubes using two different reductions from the viewpoint of geometrical stability using computerized tomography, from the point of view of mechanical properties ...
M. Ridzon +5 more
doaj
Bu makalede, AISI 1010 çelik borunun, sabit bir mandrel ile soğuk çekme işleminin benzetimi için sonlu eleman metodu kullanılmıştır. Farklı sürtünme katsayıları için, %23 kesit daralmasında yarı kalıp/mandrel açılarının çekme gerilmesi üzerine etkileri ...
Sadettin Orhan +2 more