Results 141 to 150 of about 177,448 (295)
Geometrically‐Screened, Sterically‐Hindered Additive for Wide‐Temperature Aqueous Zinc‐Ion Batteries
A molecular‑engineering strategy combining steric hindrance tuning with geometric optimization identifies cellobiose as an ideal additive for aqueous zinc‑ion batteries, enabling stable Zn deposition across a wide temperature range from −30 to 50 °C. Abstract Aqueous zinc‐ion batteries (AZIBs) are emerging as a highly promising alternative to lithium ...
Sida Zhang +13 more
wiley +1 more source
Corrosion experiments with everyday used metals [PDF]
La corrosión que sufren los metales en un ambiente húmedo es un fenómeno muy importante desde un punto de vista tecnológico, pues sus propiedades mecánicas empeoran sustancialmente al sufrir corrosión.
Heredia Avalos, Santiago
core +1 more source
Pullulan, a biomass‐derived polysaccharide, is transformed into transparent optical fibers using a solvent‐free borax hydrogel‐spinning method. The fibers outperform PMMA with ≈200 MPa tensile strength and 200 °C stability, while uniquely guiding visible‐to‐NIR light and enabling additive‐free humidity sensing.
Yuya Fukata +4 more
wiley +1 more source
In this research work, four distinct WO3 electrodes were synthesized and coated with three different polymers, known as polypyrrole (PPy), poly(3,4-ethylenedioxythiophene) in poly(4-styrenesulfonate) (PEDOT:PSS) and polyaniline (PANi), using ...
Gemma Roselló-Márquez +3 more
doaj +1 more source
Fe and P co‐doped Co9S8 nanocorals (Fe, P‐Co9S8) are successfully synthesized by a heteroatom engineering strategy, which exhibit outstanding bifunctional electrocatalytic performance for both the hydrogen evolution reaction (HER) and hydrazine oxidation reaction (HzOR).
Yuying Meng +8 more
wiley +1 more source
Efecto del tratamiento térmico en la resistencia a la corrosión de la aleación cobre- berilio C17200 [PDF]
La aleación cobre de berilio CuBe2--C17200 (CDA 172) es la aleación de cobre berilio más comúnmente utilizada y destaca por su mayor resistencia y dureza en comparación con las aleaciones de cobre comerciales. C17200 aleación contiene aprox.
Gallego Ocampo, Gerlier
core
Structural Porosity and Low Mineral Density in Enamel Rods Drive Molar Incisor Hypomineralisation
This study uses advanced imaging modalities on multiple length scales to show that molar‐incisor hypomineralization does not present as a locally homogeneous pathology. Instead, microstructural defects, characterized through non‐mineralized, protein‐rich sheaths and an altered mineral structure in between prism rods, resulting in local differences in ...
Katharina Jähn‐Rickert +14 more
wiley +1 more source
Estudio electroquímico de las interacciones formadas por el extracto activo de las hojas de Morinda citrifolia en la inhibición de la corrosión de acero estructural [PDF]
Estudio de la inhibición de la corrosión de diferentes extractos de Morinda citrifolia, en la corrosión de acero estructural AISI1045En el presente trabajo de investigación se reportan los resultados obtenidos en la actividad inhibidora a la corrosión de
FRANCO TRONCO, MARA ISABEL +1 more
core