Results 101 to 110 of about 1,306,615 (288)
Localized displacement measurements based on electronic speckle-pattern interferometry are used to obtain crack mouth opening displacement (CMOD), stress intensity factor (SIF) and T-stress values during crack growth around cold-expanded holes.
Yury Matvienko +2 more
doaj
Thermomechanical fatigue tests of laser beam powder bed fusion (PBF‐LB) Inconel 718 show that the additively manufactured material reaches almost the lifetimes of conventionally‐rolled material under no‐dwell conditions. Introducing dwell times at the maximum temperature markedly reduces the lifetimes due to pronounced grain boundary sliding associated
Stefan Guth +6 more
wiley +1 more source
This study examines how helicoidal architectures with different porosities respond to bending. Adjusting layer angle and spacing in 3D‐printed polymers reveals clear tradeoffs between stiffness, strength, and energy absorption. Experiments and simulations highlight designs that distribute stress effectively, offering pathways for optimizing lightweight
Praveenkumar Subhash Patil +2 more
wiley +1 more source
Current Status and Challenges in Data Collection for Aerospace Coatings Deposited by Plasma Spraying
An innovative approach has been integrated into the GRENAT project to optimize plasma spraying and coating performance. Raw materials are accelerated and melted in the plasma generated by torches, creating coatings. Monitoring sensors collect process data which are combined with ex situ characterization data.
Lila Randriamananjara +8 more
wiley +1 more source
Crack opening displacement (COD) on double edge notched (DEN), single edge notched (SEN) and center notched (SCN) specimens with various crack length was quantitatively analyzed by using video-microscopy for a machine-grazed paper.
Tanaka, Atsushi; id_orcid +2 more
core +2 more sources
The purpose of this paper is to research problems of cracks at a circular hole, which is a common crack configuration in aircraft structures. The Muskhelishvili complex function method and the Cauchy integral method are combined to develop crack surface ...
ZHU QingYu, SONG Bo, ZENG ZhaoYang
doaj
Scandium (Sc)‐doped AlCoCrFeMo HEA coatings are fabricated via flame spraying with 0.1, 0.3, and 0.5 wt% Sc additions. Among these, the HEA‐Sc0.3 coating exhibits the highest corrosion resistance, indicated by a more positive corrosion potential and lower current density.
Pankaj Kumar +7 more
wiley +1 more source
Critical Crack Tip Opening Displacement for X70 and X80 Steels - A Parametric Study
High strength line-pipe steels are widely used in long distance gas pipelines. Fracture toughness is one major parameter in the performance evaluation of these line-pipe steels. For high strength line-pipe steels, critical crack tip opening displacement (
Xiao Ben Liu +3 more
core +1 more source
Low‐voltage FIB‐SEM tomography combined with a image preprocessing pipeline improves phase contrast and enables reliable machine‐learning segmentation of conductive networks in lithium‐ion battery electrodes. Structural descriptors are extracted from segmented images, done semimanually and automated, and compared.
Lisa Beran +6 more
wiley +1 more source
Relationships between various definitions of the crack tip opening displacement
Published in: The crack tip opening displacement in elastic-plastic fracture mechanics (workshop on CTOD methodology, Geesthacht (DE), 23-25 April 1985), Springer-Verlag 1986Copy held by FIZ Karlsruhe; available from UB/TIB Hannover / FIZ ...
Hellmann, D. +4 more
core