Results 111 to 120 of about 302 (147)
Some Peculiarities of Using the Extended Finite Element Method in Modelling the Damage Behaviour of Fibre-Reinforced Composites. [PDF]
Kozák V, Vala J.
europepmc +1 more source
A Model to Account for the Effects of Load Ratio and Hydrogen Pressure on the Fatigue Crack Growth Behavior of Pressure Vessel Steels. [PDF]
Saxena A, Findley KO.
europepmc +1 more source
Determination of Fracture Mechanic Parameters of Concretes Based on Cement Matrix Enhanced by Fly Ash and Nano-Silica. [PDF]
Golewski GL.
europepmc +1 more source
Numerical Study of Crack Prediction and Growth in Automotive Wheel Rims. [PDF]
Montassir S +4 more
europepmc +1 more source
The Effect of Incorporating Lüders Plateau into a Plasticity Model in Predicting the Ballistic Impact Responses of 40CrNiMoA Steel Projectiles and Plates. [PDF]
Shi Y, Xiao X, Jia B, Wang Y, Li J.
europepmc +1 more source
Rejuvenation as the origin of planar defects in the CrCoNi medium entropy alloy. [PDF]
Yang Y +9 more
europepmc +1 more source
Some of the next articles are maybe not open access.
Related searches:
Related searches:
Engineering Failure Analysis, 2022
Abstract The present study aims to characterize the cracking behaviour of high-density poly-ethylene (HDPE) pipe elbow. Experimental studies were performed to determine the mechanical behaviour of HDPE and study the anisotropy of the material. Tension tests were performed on compact tension (CT) specimens to identify the toughness value, expressed by
Manel Dallali, J Capelle, Z Azari
exaly +2 more sources
Abstract The present study aims to characterize the cracking behaviour of high-density poly-ethylene (HDPE) pipe elbow. Experimental studies were performed to determine the mechanical behaviour of HDPE and study the anisotropy of the material. Tension tests were performed on compact tension (CT) specimens to identify the toughness value, expressed by
Manel Dallali, J Capelle, Z Azari
exaly +2 more sources
1992
Crack-tip opening displacement (CTOD) measurements were made 100 üm behind the crack tip on standard three-point bend specimens using a laser-based interferometric technique. Four materials (SAE-01 steel, 4340 steel, HY-100 steel, and tungsten) were tested at loading rates ranging from quasi-static (K ≈ 1 MPa∙ m½/s) to dynamic (K ≈ 106 MPa ∙ m½/s).
Wn Sharpe
exaly +2 more sources
Crack-tip opening displacement (CTOD) measurements were made 100 üm behind the crack tip on standard three-point bend specimens using a laser-based interferometric technique. Four materials (SAE-01 steel, 4340 steel, HY-100 steel, and tungsten) were tested at loading rates ranging from quasi-static (K ≈ 1 MPa∙ m½/s) to dynamic (K ≈ 106 MPa ∙ m½/s).
Wn Sharpe
exaly +2 more sources
Materials Science & Engineering A: Structural Materials: Properties, Microstructure and Processing, 2017
Abstract In order to understand and improve fracture toughness of heat affected zones (HAZs) of high-strength low alloy (HSLA) steels, complex microstructures including quasi-polygonal ferrite (QPF), acicular ferrite (AF), granular bainite (GB), bainitic ferrite (BF), and martensite-austenite (MA) constituent should be identified, quantified, and ...
S S Sohn
exaly +3 more sources
Abstract In order to understand and improve fracture toughness of heat affected zones (HAZs) of high-strength low alloy (HSLA) steels, complex microstructures including quasi-polygonal ferrite (QPF), acicular ferrite (AF), granular bainite (GB), bainitic ferrite (BF), and martensite-austenite (MA) constituent should be identified, quantified, and ...
S S Sohn
exaly +3 more sources
Cryogenics, 2015
Abstract The part-through fracture toughness ( K Ie ) and crack-tip opening displacement (CTOD, δ m ) of welded joints of aluminum alloy (AA) 20l4-T6, including the weld metal, the fusion zone (FZ), the heat-affected zone (HAZ), and the base material, were investigated at both liquid nitrogen temperature and liquid helium temperature with surface ...
Laifeng Li, Chuanjun Huang
exaly +2 more sources
Abstract The part-through fracture toughness ( K Ie ) and crack-tip opening displacement (CTOD, δ m ) of welded joints of aluminum alloy (AA) 20l4-T6, including the weld metal, the fusion zone (FZ), the heat-affected zone (HAZ), and the base material, were investigated at both liquid nitrogen temperature and liquid helium temperature with surface ...
Laifeng Li, Chuanjun Huang
exaly +2 more sources