Results 11 to 20 of about 15,584 (255)
Fractography of clinical failures of indirect resin composite endocrown and overlay restorations
OBJECTIVES Compare failure modes and fracture origins using fractography on recovered clinically fractured parts of indirect resin composite endocrowns and overlay restorations on endodontically treated teeth (ETT). METHODS Four endocrowns (3 molars, 1
Susanne Scherrer +2 more
exaly +2 more sources
The reconstitution of the history of a fatigue process is based on the knowledge of any correspondences between the morphology of the crack surface and the velocity of the crack growth (crack growth rate - CGR).
Hynek Lauschmann +3 more
doaj +2 more sources
Formability Limits, Fractography and Fracture Toughness in Sheet Metal Forming
This paper is focused on the utilisation of double edge notched tension, staggered and shear tests to determine fracture toughness and the formability limits by fracture in principal strain space.
Luis Reis +2 more
exaly +2 more sources
Forensic Fractography of Bone [PDF]
Fractography involves the study of fractures and cracks in a material in order to understand the cause of failure. Even as a complex, highly hierarchical composite, bone is a material that obeys physical laws, including cracking behavior.
Angi M. Christensen +2 more
semanticscholar +2 more sources
Quantitative prediction of fracture toughness (K Ic ) of polymer by fractography using deep neural networks [PDF]
Fracture surfaces provide various types of information about fracture. The fracture toughness , which represents the resistance to fracture, can be estimated using the three-dimensional (3D) information of a fracture surface, i.e. its roughness. However,
Yoh-ichi Mototake, Kaita Ito, M. Demura
semanticscholar +1 more source
An Al2014–alumina (Al2O3) composite’s characteristics are significantly influenced by the reinforcement particle size variation. Therefore, this study examines the microstructure, mechanical, fractography, and wear performance of an Al2014–Al2O3p ...
B. V. Murthy +10 more
semanticscholar +1 more source
The microstructure, mechanical characteristics, and tensile fractography of Al2014 alloy reinforced composites with 5 and 10% wt. % of 150 to 160 micron-sized SiC particles were investigated in this study.
H. S. Vasanth Kumar +6 more
semanticscholar +1 more source
Creep rupture properties of bare and coated polycrystalline nickel-based superalloy Rene®80 [PDF]
The mechanism governing de-oxidation of vanadium metal is regarded as fundamental knowledge; however, it has not been elucidated in existing literature.
Barjesteh M.M. +3 more
doaj +1 more source
Optimization of T-6 cycle and Characterization of Si3N4 Reinforced High Strength Aluminum Metal Matrix Composites [PDF]
In this research, AA7068/Si3N4 composites were fabricated through stir casting with the attachment of ultrasonic treatment. The quenching medium and aging duration significantly influenced the hardness of Al alloy samples.
Ashish Kumar +3 more
doaj +1 more source
TIG welding of Ti6Al4V alloy: Microstructure, fractography, tensile and microhardness data
Titanium alloy is widely used in many industries due to its unique weight to strength ratio and high corrosion resistance. A suitable method of joining Titanium and its alloys is using Tungsten Inert Gas (TIG) welding.
P. Omoniyi +3 more