Results 21 to 30 of about 15,584 (255)
The purpose of this study was to understand the behavior of martensitic H13 steel in accordance with the microstructural evolution, mechanical properties and wear in repeated tempering cycles.
Amitkumar Shelar, B. P. Ronge
doaj +1 more source
Evaluation of shear force and fractography of friction stir spot welded joints of AA 6082-T6 alloy
This experimental work investigates the tensile behavior of friction stir spot welded joints from 3 mm thick aluminum alloy AA6082-T6 sheets. Taguchi L9 Orthogonal array was used for process parameters - Tool rotational speed (TRS), Dwell time (DT) and ...
Sudhir Kumar +4 more
semanticscholar +1 more source
Today’s demand for environmentally friendly and energy-efficient solutions to the construction industry has driven researchers to match natural resources with traditional technics to develop new building technologies.
F. P. Teixeira +3 more
doaj +1 more source
Toward quantitative fractography using convolutional neural networks [PDF]
The science of fractography revolves around the correlation between topographic characteristics of the fracture surface and the mechanisms and external conditions leading to their creation.
Stylianos Tsopanidis +2 more
semanticscholar +1 more source
Effect of Boride Layer on PM HSS AISI M2 on the Mechanisms Acting in the Transverse Rupture Strength Test [PDF]
Herein, it was conducted a study in order to examine the main fracture characteristics in the transverse rupture strength test (TRS) of a high speed steel (HSS) AISI M2 produced by powder metallurgy (PM) and with boriding treatment.
Mateus Leal Arcego +3 more
doaj +2 more sources
The paper presents results of the investigations on the effect of the low-temperature thermomechanical treatment on the microstructure of AlZn6Mg0.8Zr alloy (7003 alloy) and the relationships between microstructure and fatigue properties and fractography
Aleksander Kowalski +4 more
doaj +1 more source
Cauchy-based Modelling in Cementitious Materials Technology [PDF]
Cauchy paved the way for constructing models in concrete technology, and elsewhere. He determined the (nonflat) surface area in 3D by measuring random total projections. Analogously, he determined the length of a curved line in 2D by way of measuring the
P. Stroeven, M. Słowik
doaj +1 more source
Fractography and failure mechanisms of amorphous thermoplastics
S.387-436For glassy thermoplastics during the fracture process itself, craze material is differently formed and fractured depending on microscopic parameters such as molecular weight and on macroscopic prameters such as time, crack speed and stress ...
Döll, W.
core +1 more source
A Guide to Forensic Fractography of Bone
The purpose of this guide is to familiarize the user with the science of fractography and how it can be used to examine and interpret skeletal fractures.
Angi M. Christensen +6 more
core +1 more source
Axial fully-reversed strain-controlled (R=−1) fatigue experiments were performed to obtain data demonstrating the effects of building orientation (i.e. vertical versus horizontal) and heat treatment on the fatigue behavior of 17–4 PH stainless steel (SS)
Aref Yadollahi +3 more