Results 31 to 40 of about 15,584 (255)

Evaluation of mechanical behaviour and tensile failure analysis of 8 wt.% of nano B4C particles reinforced Al2214 alloy nano composites

open access: yesManufacturing Review, 2022
The microstructure and mechanical properties of Al2214-8 wt.% of 500 nm sized B4C particles reinforced composites were studied in this study. By using a liquid metallurgical process, composites containing 8 wt.% of B4C in Al2214 alloy were created.
Gopalan Kumar   +3 more
doaj   +1 more source

The effect of platinum-aluminide coating features on high-temperature fatigue life of nickel-based superalloy Rene®80 [PDF]

open access: yesJournal of Mining and Metallurgy. Section B: Metallurgy, 2019
Low cycle fatigue is the most important failure mode in Aviation/Industrial engine rotary turbine parts. In this paper, the influence of Pt-aluminide coating parameters on high temperature low cycle fatigue behavior of superalloy Rene®80 which is used to
Barjesteh M.M.   +3 more
doaj   +1 more source

Erosive wear properties of ZA-27 alloy-based nanocomposites: Influence of type, amount, and size of nanoparticle reinforcements

open access: yesFriction, 2018
Metal matrix nanocomposites (MMnCs) comprise a metal matrix filled with nanosized reinforcements with physical and mechanical properties that are very different from those of the matrix.
Aleksandar Vencl   +5 more
doaj   +1 more source

Mechanical and tribological behavior of flyash, red mud and mica particles reinforced Al7075 alloy hybrid metal composites

open access: yesManufacturing Review, 2022
In the present research Al7075 alloy with 1, 3 and 5 varying weight percentages of flyash, 1, 2 and 3 varying wt.% of red mud along with constant 4 wt.% of mica particles composites were synthesized by stir casting technique.
Matti Siddesh   +5 more
doaj   +1 more source

Characterization of Corrosion and Stress Corrosion Cracking of AE44 Magnesium Alloy [PDF]

open access: yesArchives of Metallurgy and Materials, 2020
The paper presents the susceptibility of AE44 magnesium alloy to electrochemical corrosion and stress corrosion cracking (SCC). The evaluation of the intensity of the interaction of the corrosive environment was carried out using the corrosion tests and ...
M. Sozańska, A. Mościcki, B. Chmiela
doaj   +1 more source

Unsupervised Machine Learning in Fractography: Evaluation and Interpretation

open access: yesMaterials Characterization, 2020
Modern computer vision and machine learning techniques, when applied in Fractogra- phy bare the potential to automate much of the failure analysis process and remove human induced ambiguity or bias.
Shmuel Osovski, Stylianos Tsopanidis
semanticscholar   +1 more source

Effect of Dialkyl Peroxide Blending on Tensile Properties of PLA/PBAT Polymer Alloys

open access: yesEngineering Transactions, 2014
Poly(lactic acid) (PLA) and poly(butylene adipate/terephthalate) (PBAT) were used for polymer alloys, and the effects of the mixing ratio of PLA and PBAT and the addition of dialkyl peroxide (compatibilizing agent) were examined. The stress-strain curves
Masahiro NISHIDA   +4 more
doaj   +1 more source

Effect of Controlled Rolling and Cooling Process on Microstructures and Mechanical Properties of Low Carbon Bainitic Steel AH80DBD

open access: yesTeshugang, 2023
The effect of microstructure on impact properties of AH80DBD low carbon bainite steel is analyzed by macro-fractography, scanning fractography, metallography and transmission electron microscope.
陈尹泽, 李娜, 宋立伟, 马志强
doaj  

Eliciting stable nanoscale fracture in single-crystal silicon

open access: yesMaterials Research Letters, 2022
In this letter, we demonstrated stable nanoscale fracture in single-crystal silicon using an in-situ wedge-loaded double cantilever beam (DCB) specimen.
Frank W. DelRio   +7 more
doaj   +1 more source

A Short Review on Fracture Mechanisms of Mechanical Components Operated under Industrial Process Conditions: Fractographic Analysis and Selected Prevention Strategies

open access: yesMetals, 2019
An insight of the dominant fracture mechanisms occurring in mechanical metallic components during industrial service conditions is offered through this short overview.
George A. Pantazopoulos
doaj   +1 more source