Results 1 to 10 of about 22,691 (145)

Microstructural Evolution of Wrought-Nickel-Based Superalloy GH4169

open access: yesMetals, 2022
To investigate the microstructural evolution of wrought-nickel-based superalloy GH4169 from the original ingot to the finished product of manufacturing processes, different kinds of etchants and etching methods were used to show the fine precipitates and
Kaixuan Chen, Yuzhi Zhu, Junwei Qin
exaly   +5 more sources

Properties of GH4169 Superalloy Characterized by Nonlinear Ultrasonic Waves [PDF]

open access: yesAdvances in Materials Science and Engineering, 2015
The nonlinear wave motion equation is solved by the perturbation method. The nonlinear ultrasonic coefficients β and δ are related to the fundamental and harmonic amplitudes.
Hongjuan Yan   +3 more
doaj   +5 more sources

Influence of Precipitates on the Initial Oxidation Behavior of GH4169 Superalloy at 1000 °C

open access: yesCorrosion Communications
The degradation of mechanical properties in superalloys due to high temperature oxidation is unavoidable. In this paper, the initial oxidation (oxidation time less than 3600 s) mechanism of GH4169 superalloy was studied.
Quanxin Shi, Liuwei Zheng, Jinyao Ma
exaly   +4 more sources

Constitutive Equation of GH4169 Superalloy and Microstructure Evolution Simulation of Double-Open Multidirectional Forging

open access: yesMetals, 2019
This paper presented a double-open multidirectional forging with relatively few deformation passes and a uniform deformation. The constitutive equation and dynamic recrystallization model of the GH4169 superalloy were identified based on a thermal ...
Jun-Ting Luo, Chunxiang Zhang
exaly   +4 more sources

Behavior of Nitrogen in GH4169 Superalloy Melt during Vacuum Induction Melting Using Returned Materials

open access: yesMetals, 2021
The nitrogen behavior of superalloy melt GH4169 during the vacuum induction melting (VIM) process was clarified by using different proportions of returned materials including block-shaped returned material, chip-shaped returned material, and pure ...
Shengyong Gao   +4 more
doaj   +2 more sources

Study on the Machinability of Ni-Based Superalloy by Milling Parameters and Cooling Methods under Minimal Quantity Lubrication

open access: yesApplied Sciences, 2023
To explore the milling characteristics of Ni-based superalloy under minimal quantity lubrication (MQL), a single-factor experiment was adopted to investigate the milling machinability of GH4169 Ni-based superalloy.
Yihan Jiang   +4 more
doaj   +2 more sources

Thermal Deformation Behavior and Microstructure Evolution of GH4169 Superalloy Under the Shear-Compression Deformation Conditions

open access: yesMaterials and Design, 2021
The shear-compression deformation of GH4169 superalloy at 1000–1200 °C and 0.01–1 s−1 was investigated by physical and numerical simulation based on a specific shear-compression sample (SCS).
Luo Rui, Yu Cao, Leli Chen
exaly   +3 more sources

High Temperature Oxidation Behavior of GH4169 Nickel Base Superalloy Under Different Grindings for Internal Combustion Engine [PDF]

open access: yesCailiao Baohu, 2021
In order to improve the high temperature oxidation resistance of GH4169 nickel base superalloy for internal combustion engine, the GH4169 nickel base superalloy’s surface was polished with different types of sandpaper, and then the oxidation resistance ...
LIU Yi-fu, ZHENG Jian-xin, SUN Rui-xia
doaj   +1 more source

Investigation of microstructure and mechanical properties of GH4169 superalloy joint produced by linear friction welding

open access: yesJournal of Materials Research and Technology, 2023
Linear friction welding (LFW) method is a solid-state manufacturing process. In the present study, GH4169 superalloy was welded using LFW method. Macro morphology and shortening of LFW GH4169 joints were investigated to understand the effect of welding ...
Xiawei Yang   +8 more
doaj   +1 more source

High Cycle Fatigue Life Prediction of Single‐Crystal Specimen Based on TCD Method and Crystal Plasticity Theory

open access: yesInternational Journal of Aerospace Engineering, Volume 2023, Issue 1, 2023., 2023
This paper performs a comprehensive investigation on the high cycle fatigue (HCF) life prediction of turbine blade with film cooling holes. The modified theory of critical distance (MTCD) method is proposed to estimate the fatigue life of the specimen considering the notch sensitivity coefficient and multiaxial stress effect.
Yunwu Wu   +5 more
wiley   +1 more source

Home - About - Disclaimer - Privacy