Results 21 to 30 of about 22,691 (145)

Machining Distortion for Thin-Walled Superalloy GH4169 Caused by Residual Stress and Manufacturing Sequences

open access: yesMetals, 2022
The residual stress generated in the machining process has a passive influence on the machining accuracy of a thin-walled workpiece. Annealing treatment can release the residual stress induced in the machining process and suppress the machining ...
Pingzhong Zhu   +3 more
doaj   +2 more sources

Effect of Turning and Surface Polishing Treatments on Surface Integrity and Fatigue Performance of Nickel-Based Alloy GH4169

open access: yesMetals, 2018
In this paper, the effects of turning and surface polishing treatments on surface integrity and fatigue properties of superalloy GH4169 were investigated.
Daoxia Wu, Dinghua Zhang, Changfeng Yao
doaj   +2 more sources

Comparison of the Warm Deformation Constitutive Model of GH4169 Alloy Based on Neural Network and the Arrhenius Model

open access: yesMetals, 2022
In order to realize a better description of plastic flow behavior in the warm deformation process of GH4149, the GH4169 superalloy was compressed by Gleeble-3800 at a temperature of 700–900 °C and a strain rate of 0.01–10 s−1.
Peng Cheng   +4 more
doaj   +2 more sources

Numerical Simulation of Hot Forging for the Disc of Superalloy GH4169

open access: yesAdvanced Materials Research, 2011
In this paper, the hot deformation behavior of GH4169 superalloy were investigated at temperature of 900-1020°C and at strain rate of 0.001-0.1up to a 60% height reduction of the sample using isothermal constant strain rate compression tests on process annealed material.
Yan Shu Zhang, Xiao Fei Liu
openaire   +2 more sources

Surface oxidation characteristics of nickel-base superalloy GH4169 powder

open access: yesJournal of Aeronautical Materials, 2020
The effect of temperature on surface oxidation characteristics of nickel-base superalloy GH4169 powder was investigated by field emission scanning electron microscope (FE-SEM),energy-dispersive spectroscopy (EDS),X-ray photoelectron spectroscopy (XPS ...
Zhang Lichong   +6 more
doaj   +2 more sources

Effect of holding time and AgCuTi composite filler on microstructure and mechanical properties of GH4169/SiC vacuum brazed joints

open access: yesMaterials Research Express
The GH4169 superalloy and SiC ceramic were joined via vacuum brazing using AgCuTi filler and AgCuTi + Cu foam composite filler, respectively, to investigate their joint properties. The influence of holding time on the microstructure and shear strength of
Wei Wang, Liangping Cheng, Chao Cui
doaj   +2 more sources

Microstructure and Creep Property of a GH4169 Nickel-based Superalloy

open access: yesCailiao gongcheng, 2017
By means of direct aging (DA) heat treatment, creep properties measurement and microstructure observation, the microstructure and creep behaviors of the GH4169 superalloy were investigated. Results show that the microstructure of the alloy consists of γ, γ', γ" and δ phases, and the coherent interfaces exist between the phases.
LIU Chen   +4 more
openaire   +3 more sources

Thermodynamic Entropy-Based Fatigue Life Assessment Method for Nickel-Based Superalloy GH4169 at Elevated Temperature Considering Cyclic Viscoplasticity

open access: yesEntropy
This paper develops a thermodynamic entropy-based life prediction model to estimate the low-cycle fatigue (LCF) life of the nickel-based superalloy GH4169 at elevated temperature (650 °C). The gauge section of the specimen was chosen as the thermodynamic
Shuiting Ding   +6 more
doaj   +2 more sources

A Novel Method for Predicting Residual Stress in GH4169 Machined Surfaces through Micro-Hardness Measurement

open access: yesApplied Sciences, 2023
The presence of residual stress seriously affects the mechanical performance and reliability of engineering components. Here, the authors propose a novel method to determine corresponding residual stress through micro-hardness measurements of machined ...
Gonghou Yao, Zhanqiang Liu, Haifeng Ma
doaj   +2 more sources

Experimental Study on Thermostatic Cutting Nickel-Base Superalloy GH4169

open access: yesAdvanced Materials Research, 2010
Nickel-base super alloy GH4169 is difficult to cutting and tool wear is very serious, because of its high strength, poor thermal conductivity, and serious work-hardening. In order to choose reasonable cutting parameters as to improve the processing efficiency, the cutting experiments were crarried out and the changes of workpiece material physical in ...
Zhao Peng Hao, R.D. Han, D. Gao
openaire   +2 more sources