Results 41 to 50 of about 22,691 (145)

Pore structure and performance of porous GH4169 superalloys preparedby laser additive manufacturing

open access: yesFenmo yejin jishu, 2023
Porous GH4169 superalloy materials with the different pore structures were prepared by selective laser melting technology. The effects of pore structure on the capillary and compressive mechanical properties were investigated by scanning electron ...
LIANG Jiamiao   +5 more
doaj   +1 more source

Thermal Mismatch Effect and High‐Temperature Tensile Performance Simulation of Hybrid CMC and Superalloy Bolted Joint by Progressive Damage Analysis

open access: yesInternational Journal of Aerospace Engineering, Volume 2020, Issue 1, 2020., 2020
The hybrid CMC and superalloy bolted joints have exhibited great potential to be used as thermostructural components of reusable space transportation systems, given the respective strengths of these two materials. In the high temperature excursion of the hybrid joints with the aircrafts and space vehicles, the substantial difference in thermal ...
Shuyuan Zhao   +6 more
wiley   +1 more source

Development and Characterization of ZnO Piezoelectric Thin Film Sensors on GH4169 Superalloy Steel Substrate by Magnetron Sputtering

open access: yesMicromachines, 2022
At present, piezoelectric sensors are primarily applied in health monitoring areas. They may fall off owing to the adhesive’s durability, and even damage the monitored equipment.
Guowei Mo   +3 more
doaj   +1 more source

Effect of heat input on microstructure and mechanical properties of GH159 and GH4169 dissimilar joints by laser beam welding

open access: yesMaterials Research Express, 2021
Co-based superalloy GH159 and Ni-based superalloy GH4169 have been successfully joined by laser beam welding and the effect of heat input on microstructure and properties of dissimilar joints were investigated systematically. The results showed that weld
Qian Ran   +3 more
doaj   +1 more source

Non-Unified Constitutive Models for the Simulation of the Asymmetrical Cyclic Behavior of GH4169 at Elevated Temperatures

open access: yesMetals, 2022
The tensile, creep, fatigue and creep-fatigue tests of the nickel-based superalloy GH4169 were carried out. According to the deformation characteristics of GH4169 alloy, the Ohno-Karim kinematic model (O-K model) can be used to describe the tensile ...
Xuteng Hu   +4 more
doaj   +1 more source

Multistage fatigue modeling of single-edge-notch tension specimens for Ni-based superalloy GH4169

open access: yesAdvances in Mechanical Engineering, 2017
Multistage fatigue tests were conducted on the single-edge-notch tension specimens of Ni-based superalloy GH4169. Fatigue crack growth data at different stages were recorded with the surface replica technique.
ZR Wu, FL Liu, X Li, L Fang, YD Song
doaj   +1 more source

Evaluation of multiaxial fatigue life prediction criteria for Ni-based superalloy GH4169

open access: yes, 2017
Fatigue tests under multiaxial loading were conducted on Ni-based superalloy GH4169 tubular specimens. The microstructures of fracture surfaces under different loading paths were compared.
YD Song, ZR Wu, L Fang, X Li
core   +1 more source

Effect of temperature on the creep behavior and mechanism of GH4169 alloy

open access: yes工程科学学报, 2023
GH4169, a precipitation-strengthened nickel-based superalloy, has been extensively used in structural applications in temperatures up to 650 ℃ because of its high-temperature strength, long-term stability, thermal fatigue, creep resistance, corrosion ...
Sheng-yong GAO   +4 more
doaj   +1 more source

Study of Manufacturing Process of Holes in Aeroengine Heat Shield

open access: yesInternational Journal of Aerospace Engineering, Volume 2019, Issue 1, 2019., 2019
The nickel‐based superalloy GH3128 with high plasticity, high long‐lasting creep strength, good resistance to oxidation and stamping, and good welding performance is widely used in aircraft engine heat shields. The many holes that need to be machined on the heat shield are not only small in diameter but also dense, and GH3128 as a typical hard‐to ...
Anyuan Jiao   +2 more
wiley   +1 more source

A Modified Walker Model Dealing with Mean Stress Effect in Fatigue Life Prediction for Aeroengine Disks

open access: yesMathematical Problems in Engineering, Volume 2018, Issue 1, 2018., 2018
Mean stress effect plays an important role in fatigue life prediction, and it is discovered that maximum stress has nonnegligible influence on mean stress effect. Therefore, a modified Walker model is proposed to account for mean stress effect on fatigue life of aeroengine disks, which contains the influence of stress ratio and maximum stress on mean ...
Shan Lu   +4 more
wiley   +1 more source

Home - About - Disclaimer - Privacy