Results 51 to 60 of about 22,691 (145)
ABSTRACT Nickel‐based superalloys (Ni‐based superalloys) have attracted extensive attention in laser additive manufacturing (LAM) due to their capability to directly fabricate complex and high‐performance structural components. However, the rapid melting and solidification inherent to LAM result in intense thermal cycling, which induces high residual ...
Tianxiang Lin +9 more
wiley +1 more source
Reliability Analysis on Structures Based on a Modified Iterative Response Surface Method
In order to improve the computational accuracy and efficiency of response surface method for reliability analysis on structures, a modified iterative response surface method (called as NDIRSM) is proposed. Firstly, a new starting center point, which is closer to design point, is calculated out as the starting center point instead of the point at mean ...
Yanxu Wei +4 more
wiley +1 more source
A novel machine learning strategy tackles ambiguous compositional data to predict superalloy fatigue. By integrating partial label with transfer learning and enriching features through thermodynamic calculations, this approach achieves superior accuracy and interpretability.
Haopeng Lv +10 more
wiley +1 more source
Surface Microstructure of Nanoaluminized CoCrAlY Coating Irradiated by HCPEB
A thermal sprayed CoCrAlY coating was prepared by air plasma spray on the surface of Ni‐based superalloy GH4169; then, a nanoscale aluminum film was deposited with electron beam vacuum deposition on it. The coatings irradiated by high‐current pulsed electron beam were investigated. After HCPEB treatment, the Al film was remelted into the bond coat. XRD
Zhiyong Han +3 more
wiley +1 more source
The diffusion multiple technique enables the simultaneous diffusion of various elements within a single sample preparation, and the characterization of the microstructural morphology and mechanical properties in the diffusion region can facilitate the rapid screening of alloy compositions.
Haoyan Meng +9 more
wiley +1 more source
Performance of two different constitutive models and microstructural evolution of GH4169 superalloy
The hot compression tests of GH4169 superalloy were performed in the deformation temperature range of 970 to 1150 ℃ and at the strain rate range of 0.001 to 10 s⁻¹. The flow stress is dependent on temperature and strain rate. The flow stresses were respectively predicted by Arrhenius-type and artificial neural network (ANN) models, and the predicted ...
Xiawei Yang +5 more
openaire +3 more sources
Experimental on ultrahigh frequency vibration fatigue of GH4169 nickel-based superalloy
To address the very high cycle fatigue(VHCF)issue of GH4169 nickel-based superalloy,which is widely utilized in aero-engines,a fatigue specimen subjected to 20 kHz ultrahigh frequency vibration is designed and tested utilizing a piezoelectric ultrasonic ...
WANG Zhaohan +5 more
doaj +1 more source
Roughness Prediction and Performance Analysis of Data-Driven Superalloy Belt Grinding
Abrasive belt grinding has unique advantages in avoiding machining defects and improving surface integrity while grinding hard materials such as superalloys.
Youdong Zhang +5 more
doaj +1 more source
Machine Learning‐Assisted Sensitivity Analysis for Stochastic Fatigue Life Modeling of Metals
ABSTRACT Predicting fatigue life with precision requires more than isolated evaluations of mechanical properties; it requires an integrated approach that captures the interdependencies between various parameters, including elastic modulus, tensile strength, yield strength, and strain‐hardening exponent.
Tran C. H. Nguyen, N. Vu‐Bac
wiley +1 more source
Numerical Simulation of Creep Damage and Life Prediction of Superalloy Turbine Blade
Creep caused failure is an important failure mode of the turbine blade. A numerical approach of life assessment of the superalloy turbine blade is proposed in the present paper based on the Lemaitre‐Chaboche creep damage model. Material damage is introduced into each element based on the ANSYS APDL function, and the creep damage effect is considered ...
Donghuan Liu +3 more
wiley +1 more source