Results 61 to 70 of about 22,691 (145)
ABSTRACT Hot‐forged wheel bearing hubs are manufactured using a complicated fabrication process chain to obtain the desired microstructure and mechanical properties in different zones that experience varying local stress states. The different process steps modify the surface roughness and the residual stresses distribution and therefore affect the ...
Vo‐Huu‐Thuc Nguyen +6 more
wiley +1 more source
Experimental study of picosecond laser-assisted grinding of GH4169 nickel-based superalloy [PDF]
The nickel-based superalloy GH4169 exhibits excellent thermal stability and fatigue resistance, making it widely utilized in the aerospace and marine manufacturing industries.
Tang, X +7 more
core +1 more source
A Review of High‐Temperature Molten Salt for Third‐Generation Concentrating Solar Power
Our review explores molten salts suitable for third‐generation concentrating solar power (CSP) systems, focusing on carbonates, chlorides, and sulfates. We examine their thermal properties and explore how nanoparticles enhance their heat storage capacity.
Xu Liu +4 more
wiley +1 more source
Effects of Pulse Current on Dynamic Recrystallization Behavior of GH4169 Superalloy
The pulse current was applied on the GH4169 alloy during tensile tests at 800°C. The effects of pulse current on the deformation behavior and recrystallization of the alloy were investigated, and the mechanisms were also discussed. The results show that the deformation resistance decreases and the elongation increases significantly by applying the ...
Liu, Yang +4 more
openaire +2 more sources
Theoretical and Experimental Research on Tapping Forces of Nickel-Based Superalloy GH4169
The mechanical model of the tapping torque and the friction one were established based on Theoretical Research of Tapping Forces. A series of standard taps with a cutting cone angle of 7°30′ were prepared from high-speed steel W9 and used to tap Nickel ...
Rong Di Han, Lin Geng, Y.L. Tang
core +1 more source
Laser shock peening (LSP), as an innovative surface treatment technology, can effectively improve fatigue life, surface hardness, corrosion resistance, and residual compressive stress. Compared with laser shock peening, warm laser shock peening (WLSP) is
Wu, Jiajun +15 more
core +2 more sources
Rolling is a process that can improve the performance and roughness of machined parts and has a special economic value; therefore, the optimization of rolling process parameters is crucial to workpiece performance.
Fang Yu, Jiachun Li
doaj +1 more source
The mechanical properties of GH4169 alloy sheet after cold rolling (at 0%, 10%, 30%, 50% and 70%) and solid solution were investigated. The textures and Taylor factors were characterized using electron backscattering diffraction (EBSD).
Shi-Hong Zhang +5 more
doaj +1 more source
Mechanical Properties of GH4169 superalloy Prepared by Selective Laser Melting
Using selective laser melting technique, 3 sets of GH4169 samples were formed by various laser power and scanning speed to prepare mechanical properties test specimens. The defects and porosity of the samples were measured by CT inspection. The tensile test was carried out at room temperature. The fracture morphology of the tensile samples was observed
Guohui Zhang +6 more
openaire +1 more source
A series of strain-controlled creep-fatigue tests under different loading waveforms are carried out on GH4169 superalloy at 650 °C. In the macroscopic view, a unified viscoplastic constitutive framework is used to describe cyclic deformation process ...
Run-Zi Wang +4 more
doaj +1 more source