Results 21 to 30 of about 8,464 (186)
Abrasive wear resistance of a quenched and sub-zero treated high-chromium white cast iron
The study reported in this paper concerned development of such microstructure of high-chromium (24 % Cr) cast iron which could secure high abrasive wear resistance of die inserts used to fabricate stampings from refractory materials. It was found that by
A. W. Orłowicz +5 more
doaj +2 more sources
The study investigated the microstructure and mechanical properties of composite strengthened high-chromium cast iron by laser quenching and laser shock peening.
Aixin Feng +5 more
doaj +1 more source
TiC reinforced high chromium cast iron(HCCI) matrix composites were prepared by high energy ball milling and vacuum sintering.Scanning electron microscope (SEM) and differential scanning calorimetry (DSC) were employed to analyze the powder at different ...
XU Jiahao, WANG Xuanguo, YAO Zhenhua
doaj +1 more source
Purpose. The article is aimed to obtain the regression dependences of manganese distribution between carbides and the metal base on the content of pig iron C, Cr, Mn and Ni after annealing at 690°C. Methodology.
V. V. Netrebko
doaj +1 more source
Study on Microstructure and Hot Deformation Behavior of High Chromium Cast Iron/Low Carbon Steel Laminate [PDF]
A hot compression process was developed to study the hot deformation behavior and microstructure of a high chromium cast iron/low carbon steel laminate on a Gleeble 3800 thermal simulation test machine at a temperature of 950-1200℃.
G. Yuan +5 more
doaj +1 more source
Analysis of Carbides in Multi-component Cast Iron Design Based on High Entropy Alloys Concepts [PDF]
Nowadays, the concept of high entropy alloys (HEAs) has expanded the limits of metallurgy and high-quality metallurgical HEAs ingots have already been successfully obtained on an industrial scale.
W. M. Pasini +4 more
doaj +2 more sources
Effect of Subcritical Treatment (Tempering) on Hardness and Wear of High Chromium White Cast Iron [PDF]
High chromium white cast iron (HCWCI) is used in mining, crushing plants, as mill liners, and in the manufacture of grinding balls. The grinding ball is the essential element in fine fragmentation.
Sahraoui Aissat, Ali Safa
doaj +1 more source
Abrasion Resistance of as-Cast High-Chromium Cast Iron
Abstract High chromium cast irons are widely used as abrasion resistant materials. Their properties and wear resistance depend on carbides and on the nature of the matrix supporting these carbides. The paper presents test results of irons which contain (in wt.%) 18-22 Cr and 2-5 C, and is alloyed by 1.7 Mo + 5 Ni + 2 Mn to improve the ...
Marcela Pokusová +2 more
openaire +1 more source
A probabilistic model for the high cycle fatigue behaviour of cast aluminium alloys subject to complex loads [PDF]
Lien vers la version éditeur: http://www.sciencedirect.com/science/article/pii/S0142112312002472This article is dedicated to the high cycle fatigue behaviour of cast hypo-eutectic Al–Si alloys and in particular the AlSi7Cu05Mg03 alloy.
PESSARD, Etienne +3 more
core +1 more source
Effect of High-Temperature Quenching on the Phase Composition, Structure, and Wear Resistance of Ni-Hard Chromium-Nickel Cast Iron [PDF]
Metallographic, micro-X-ray spectral and X-ray structural analyses have been carried out. The quenching temperature increase from 900 to 1150 °C leads to high abrasive wear resistance in Ni-hard chromium-nickel cast iron.
Filippov M.A. +3 more
doaj +1 more source