Effect of Aggregate Gradation on Workability of Hot Mix Asphalt Mixtures
The ease of hot mix asphalt (HMA) mixture for compacting describes workability of the HMA mixture. This study developed a simple workability index (WI) and applied it to investigate effect of aggregate gradation on workability of HMA mixtures.
Iman Haryanto, Osamu Takahashi
doaj
Hot Workability for a Ti-Nb IF Steel in Ferrite Area
According to hot simulation test results by Gleeble 1500D machine, the analytic expression between flow peak stress σpand Zener-Hollomon factor Z ( T, ε ) for Ti-Nb IF ( interstitial atom free) steel (0. 005C, 0. 055Al, 0. 01 Nb, 0.
张鹏, 汪凌云, 李伟
doaj
REINFORCEMENT AND HOT WORKABILITY OF ALUMINIUM ALLOY 7075 PARTICULATE COMPOSITES: A REVIEW [PDF]
A proper selection of matrix and reinforcement result in the best combinations of physical and mechanical properties in the resulting a metal matrix composite (MMC).
Q. M. AZPEN +3 more
doaj
Evaluation of Hot Workability of Nickel-Based Superalloy Using Activation Energy Map and Processing Maps. [PDF]
Lypchanskyi O +4 more
europepmc +1 more source
Hot Workability of Ultra-Supercritical Rotor Steel Using a 3-D Processing Map Based on the Dynamic Material Model. [PDF]
Chen X, Du Y, Lian T, Du K, Huang T.
europepmc +1 more source
A Study on Hot Workability of Super Duplex Stainless Steel 00Cr25Ni7Mo4N
Test of tensile properties and compression with single pass and continuous 4 pass at elevated temperature for forged bar of steel 00Cr25Ni7Mo4N melted by vacuum induction funace has been carried out by Gleeble thermal simulator.
王晓峰, 陈伟庆, 宋红梅
doaj
Hot-Workability of IN706 Alloy
Z. Long, D. Fu, Z. Zhong, P. Ma
openaire +1 more source
A Study on Hot Workability of Corrosion Resistance Alloy G3,G3-Z and 825
The stress-strain curves of corrosion resistant alloys G3 (%:0.012C,46.51Ni,24.71Cr,8.88Mo, 1.15W,1.72Cu,0. 10Nb),G3-Z(%:0.014C,46.53Ni,24.05Cr,6.89Mo,1.09W,1.70Cu)and alloy 825(%: 0.006C,43.77Ni,22.
包耀宗 +5 more
doaj
Influence of Cerium on Hot Workability of Super Duplex Stainless Steel 00Cr25Ni7Mo4N
Hot tension test with strain rate 5×10-3s-1and hot reduction test with deformation 60% and strain rate 1×100s-1for 0~0.034% Ce super duplex stainless steel 00Cr25Ni7Mo4N (%:0.016~0.020C,24.50~24.72Cr, 7.06~7.
俞飞 +5 more
doaj
Hot Workability of Ti-6Al-4V Alloys
Hirowo G. SUZUKI +4 more
openaire +2 more sources