Results 41 to 50 of about 4,288,982 (141)

Light beam induced current of light-induced degradation in high-performance multicrystalline Al-BSF cells

open access: yes, 2022
99106Multicrystalline silicon solar cells are plagued by different types of light-induced degradation (LID), including Sponge-LID. Sponge-LID decreases the Al-BSF cell efficiency by up to 10 %rel. and is only partially recoverable at 200°C.
Rinio, M.   +5 more
core   +1 more source

Reduction in the short-circuit current density of silicon heterojunction photovoltaic modules subjected to potential-induced degradation tests [PDF]

open access: yes, 2016
This letter deals with the potential-induced degradation (PID) of silicon heterojunction(SHJ) photovoltaic (PV) modules. After rapid indoor PID tests applying a voltage of −1000 V at 85 ◦C, the modules exhibited a significant reduction in short-circuit ...
Masuda, Atsushi   +3 more
core   +1 more source

Material Collected From the Induced Seismicity State Task Force Meeting, Wednesday, April 16, 2014, Newman University, Wichita, Kansas

open access: yes, 2014
Announcement -- Agenda -- Breakout Sessions: Questions and Responses -- An Ounce of Understanding is Worth a Pound of Cure / by Kyle E. Murray -- Induced Seismicity and the Oil and Gas Industry -- Overview of Kansas Earthquakes / Rick Miller, Shelby ...
Induced Seismicity State Task Force Meeting (2014 : Wichita, Kan.)
core   +1 more source

Regulation of ErbB2 receptor status by the proteasomal DUB POH1.

open access: yesPLoS ONE, 2009
Understanding the factors, which control ErbB2 and EGF receptor (EGFR) status in cells is likely to inform future therapeutic approaches directed at these potent oncogenes.
Han Liu   +3 more
doaj   +1 more source

Regression of lid-induced corneal topography changes after reading

open access: yes, 2005
Purpose. The purpose of this article is to investigate the magnitude of lid-induced corneal topography changes as a function of time spent reading and the subsequent time course of regression of these changes. \ud Methods.
TOBIAS BUEHREN   +9 more
core   +1 more source

Formation kinetics of copper-related light-induced degradation in crystalline silicon [PDF]

open access: yes, 2014
Light-induced degradation (LID) is a deleterious effect in crystalline silicon, which is considered to originate from recombination-active boron-oxygen complexes and/or copper-related defects.
Lindroos, Jeanette   +5 more
core   +1 more source

Understanding the mechanisms of light-induced degradation in crystalline silicon [PDF]

open access: yes, 2020
The boron-oxygen-related light-induced degradation (BO-LID) and light- and elevated temperature-induced degradation (LeTID) are two common types of light-induced degradation (LID) in silicon solar cells that significantly impact performance.
Kim, Moonyong
core   +1 more source

lid-driven-cavity_gpu v1.0

open access: yes, 2016
<p>Solves lid-driven cavity problem using finite difference method on GPU, with equivalent CPU version for comparison.</p ...
Kyle Niemeyer (5253598), Kyle Niemeyer
core   +1 more source

Comprehensive study of potential‐induced degradation in silicon heterojunction photovoltaic cell modules [PDF]

open access: yes, 2018
Accelerated tests were used to study potential-induced degradation (PID) in photovoltaic (PV) modules fabricated from silicon heterojunction (SHJ) solar cells containing tungsten-doped indium oxide (IWO) transparent conductive films on both sides of the ...
Masuda, Atsushi   +7 more
core   +1 more source

Microstructural identification of Cu in solar cells sensitive to light-induced degradation

open access: yes, 2022
Art. 1600426, 5 S.Light-induced degradation (mc-LID or LeTID) can lead to a severe efficiency loss in multi-crystalline solar cells. The underlying mechanism clearly distinguishes from known mechanisms as B-O-LID and Fe-B-LID.
Hagendorf, C.   +3 more
core   +1 more source