Results 131 to 140 of about 92,782 (258)

Impact of MgO Additions on the Oxidation Resistance and Compression Behavior of Vanadium Alloys

open access: yesAdvanced Engineering Materials, EarlyView.
An increase in oxidation resistance at 600 °C is achieved for alloys containing more than 2.5 wt.% MgO. It has been established that, along with V2O5, MgO6V2, and Mg2O7V2 are formed, which are presumed to enhance oxidative stability. Furthermore, the possible transformation of Mg‐vanadates through reaction with CO2, which presumably occurs in this ...
Ievgen Solodkyi   +5 more
wiley   +1 more source

On the Effect of Creep on Local Lattice Orientation in Single‐Crystal Ni‐Based Superalloy Microstructures

open access: yesAdvanced Engineering Materials, EarlyView.
During creep of a single‐crystal Ni‐based superalloy, the overall crystal orientation is observed to remain constant while the microstructure evolves. Despite the lack of macroscopic rotation, small (<1°) rotations are observed on the submicron size scale and are accommodated by counteracting rotations over the scale of several micrometers.
E. J. Payton   +3 more
wiley   +1 more source

Distinct Microstructural Characteristic Lengths Defining Notch Fatigue Crack Initiation and Propagation, and Defect Tolerance in Advanced Steels

open access: yesAdvanced Engineering Materials, EarlyView.
Schematic representation of modes of microcrack nucleation, growth and temporary arrestment at different boundaries, with the criteria for crack propagation in three scenarios: (1) large notch, (2) defect/small sharp notch, and (3) long crack. This work revisits and integrates results on the fatigue behavior of advanced bainitic steels (in particular ...
Lucia Morales‐Rivas
wiley   +1 more source

Multilayer Self‐Limiting Electrospray Deposition via Stepped Voltage Bias

open access: yesAdvanced Engineering Materials, EarlyView.
Self‐limiting electrospray deposition (SLED) uses a high voltage to generate and deposit a charged payload on a target surface. The coating retains its charge, repelling newly arriving material. SLED thickness can be decreased by applying a secondary bias to the target.
Madhuri Deb   +3 more
wiley   +1 more source

Microstructure Modification of Additively Manufactured Mo–9Si–8B by Annealing and Its Effects on High‐Temperature Mechanical Properties

open access: yesAdvanced Engineering Materials, EarlyView.
Postbuild annealing systematically modifies the phase fractions and morphology of EB‐PBF processed Mo–9Si–8B. Quantitative microstructure–property correlations reveal how controlled phase evolution enhances high‐temperature compressive strength and creep resistance.
Christopher Schmidt   +5 more
wiley   +1 more source

Home - About - Disclaimer - Privacy