Results 221 to 230 of about 81,280 (285)
Some of the next articles are maybe not open access.
Injection molding metallic glass
Scripta Materialia, 2009Advances in alloy development have produced the Zr_(35)Ti_(30)Be_(27.5)Cu_(7.5) alloy with a crystallization–glass transition temperature, ΔT, of 165 °C. This alloy’s large supercooled liquid region provides the longest processing times and lowest processing viscosities of any metallic glass and was injection molded using tooling based on plastic ...
Wiest, Aaron +4 more
openaire +2 more sources
Fabrication of TiAl alloys turbocharger turbine wheel for engines by metal injection molding
, 2021The TiAl turbine wheels possess high acceleration responsiveness and low energy consumption due to its low density, high specific strength and excellent oxidation resistance.
Liu Yanjun +8 more
semanticscholar +1 more source
Powders for metal injection molding
Journal of the European Ceramic Society, 1998Metal injection molding (MIM) uses powders which differ considerably from the ceramics powders used for ceramic injection molding. Metal powders are hardly available in the sub-micron ranges that are almost standard in ceramics. The reason for this lies in the ductility and reactivity of the metals which make it difficult and very expensive to produce ...
T. Hartwig +5 more
openaire +1 more source
Applied Sciences
The applications of Nd-Fe-B-based magnets are experiencing significant diversification to achieve efficiency and miniaturization in different technologies.
Vahid Momeni +8 more
semanticscholar +1 more source
The applications of Nd-Fe-B-based magnets are experiencing significant diversification to achieve efficiency and miniaturization in different technologies.
Vahid Momeni +8 more
semanticscholar +1 more source
Metal Injection Molding (MIM) Processing
2015Complex-shaped components can be obtained by net or near-net shaping through the powder metallurgy processing route such as metal injection molding (MIM) process. MIM is an advanced powder processing technique for the mass production of complex-shaped components.
Hideshi Miura +2 more
openaire +1 more source
, 2020
The use of feedstocks from metal injection molding (MIM) for the additive manufacturing (AM) of green parts, which are then debound and sintered in a process called shaping, debinding, and sintering (SDS), is promising in terms of production costs of ...
L. Waalkes +3 more
semanticscholar +1 more source
The use of feedstocks from metal injection molding (MIM) for the additive manufacturing (AM) of green parts, which are then debound and sintered in a process called shaping, debinding, and sintering (SDS), is promising in terms of production costs of ...
L. Waalkes +3 more
semanticscholar +1 more source
A variotherm mold for micro metal injection molding
Microsystem Technologies, 2005In this paper, a variotherm mold was designed and fabricated for the production of 316L stainless steel microstructures by micro metal injection molding (μMIM). The variotherm mold incorporated a rapid heating/cooling system, vacuum unit, hot sprue and cavity pressure transducer. The design of the variotherm mold and the process cycle of μMIM using the
G. Fu +5 more
openaire +1 more source
, 2020
316 L stainless steel samples are fabricated using metal injection molding in which water atomized 316 L powder containing 4200 ppm oxygen is used as the raw material. Oxygen not only hampers the sintering process but also proves to be detrimental to the
Kaiping Yu +7 more
semanticscholar +1 more source
316 L stainless steel samples are fabricated using metal injection molding in which water atomized 316 L powder containing 4200 ppm oxygen is used as the raw material. Oxygen not only hampers the sintering process but also proves to be detrimental to the
Kaiping Yu +7 more
semanticscholar +1 more source
Microstructures and magnetic properties of Fe-35%Co alloy fabricated by metal injection molding
Journal of Magnetism and Magnetic Materials, 2020Annular samples are fabricated by metal injection molding using pre-alloyed Fe-35%Co powder. Samples sintered at different temperatures (1275, 1300, 1325, 1350 and 1375 °C) all exhibit a single α-FeCo solid solution phase and have low interstitial ...
Yongyun Zhang +5 more
semanticscholar +1 more source
, 2020
Impurities, particularly oxygen, are a critical issue to address in metal-injection-molding (MIM) processed Ti-Nb-Zr biomaterials. The addition of rare earth (RE) elements such as yttrium is a possible solution to the impurity problem due to their ...
P. Xu +4 more
semanticscholar +1 more source
Impurities, particularly oxygen, are a critical issue to address in metal-injection-molding (MIM) processed Ti-Nb-Zr biomaterials. The addition of rare earth (RE) elements such as yttrium is a possible solution to the impurity problem due to their ...
P. Xu +4 more
semanticscholar +1 more source