Results 31 to 40 of about 78,148 (234)

Static grain growth in an austenitic stainless steel subjected to intense plastic straining [PDF]

open access: yes, 2014
The post-dynamic recrystallization of an ultrafine grained 304-type austenitic stainless steel was studied during annealing at 800 and 1000°C for 7.5 to 480 minutes.
Belyakov, A.   +2 more
core   +1 more source

Effect of multidirectional forging and equal channel angular pressing on ultrafine grain formation in a Cu-Cr-Zr alloy [PDF]

open access: yes, 2014
The microstructure evolution was investigated in a Cu-0.3%Cr -0.5%Zr alloy subjected to large plastic deformation at temperature of 400° C. Two methods of large plastic deformation, i.e., equal channel ang ular pressing (ECAP) and multidirectional ...
Belyakov, A.   +2 more
core   +1 more source

Σ3 CSL boundary distributions in an austenitic stainless steel subjected to multidirectional forging followed by annealing [PDF]

open access: yes, 2014
The effect of processing and annealing temperatures on the grain boundary characters in the ultrafine-grained structure of a 304-type austenitic stainless steel was studied.
Andrey Belyakov   +5 more
core   +1 more source

Ultrafine grain development in copper during multidirectional forging at 195 K

open access: yesPhilosophical Magazine Letters, 2007
Strain-induced evolution of ultrafine grains in pure copper was studied in multidirectional forging (MDF) at 195 K. The stress–strain behaviour was characterized by rapid strain hardening during early processing and the rate of strain hardening gradually decreased with straining, leading to an apparent steady-state flow at large cumulative strains of ...
C. Kobayashi   +3 more
openaire   +1 more source

Forgeability of AZ Series Magnesium Alloy produced by Twin Roll Casting [PDF]

open access: yes, 2017
Plastic forming of magnesium alloy is hardly reported because of its low forgeability. The productions of magnesium alloy are mainly produced by casting. Typical wrought magnesium alloy is AZ31.
Aoki, A. (Atsuhiro)   +11 more
core   +1 more source

Anisotropic Phase Transformation Mechanism on Coarse-Grained and Fine-Grained Pure Titanium at Low-Temperature Plasma Nitriding

open access: yesУспехи физики металлов, 2022
The nitriding process of the coarse-grained and fine-grained pure titanium proceeded by multidirectional forging technique has been investigated at temperatures of 623, 673, and 723 K.
J. M. Windajanti, M. S. Rajapadni, D. J. D. H. Santjojo, M. A. Pamungkas, A. Abdurrouf, and T. Aizawa
doaj   +1 more source

Microstructural evolution of Mg-7Al-2Sn Mg alloy during multi-directional impact forging

open access: yesJournal of Magnesium and Alloys, 2015
Multi-directional impact forging (MDIF) was applied to a Mg-7Al-2Sn (wt.%) Mg alloy to investigate its effect on the microstructural evolution. MDIF process exhibited high grain refinement efficiency.
M.G. Jiang, H. Yan, L. Gao, R.S. Chen
doaj   +1 more source

Effect of forging steps on microstructure evolution and mechanical properties of Ti-6Al-4V alloy during multidirectional isothermal forging

open access: yesProcedia Manufacturing, 2020
Abstract In this study, the multidirectional isothermal forging (MDIF) was used to modify the β transformed microstructure into an equiaxed α+β structure in Ti-6Al-4V alloy. After two steps forging, the initial β grains were nearly disappeared.
Zhixiong Zhang, Tao Wang, Peng Lin
openaire   +1 more source

Grain refinement of magnesium alloys by dynamic recrystallization (DRX): A review

open access: yesJournal of Materials Research and Technology, 2023
For elevated-temperature thermomechanical processing, the occurrence of recrystallization during straining is known as dynamic recrystallization (DRX), which usually happens in Mg alloys during practical hot deformation processes such as rolling, forging,
Hamed Mirzadeh
doaj   +1 more source

Ultrafine-grained structure formation in Ti-6Al-4V alloy via warm swaging [PDF]

open access: yes, 2014
The influence of warm swaging on the structure and properties of Ti-6Al-4V alloy was studied. Warm swaging of the alloy in the interval 680-500°C with the total strain of ε=2.66 was found to be resulted in the formation of a homogeneous globular ...
Klimova, М.   +2 more