Hardness, Microstructure and Strain Distributions in Commercial Purity Aluminum Processed by Multi Directional Forging (MDF) [PDF]
Severe plastic deformation (SPD) of metals leads to their strengthening and grain refinement, but to low uniform elongations. Low Strain Amplitude Multi Directional Forging (LSA-MDF) is an important method for increasing this low uniform elongation.
Natanael Geraldo Silva Almeida +5 more
doaj +5 more sources
Microstructural refinement and mechanical property enhancement of AZ91 magnesium alloy via room-temperature multi-directional forging [PDF]
This study investigates the microstructural transformation and mechanical behavior of an AZ91 magnesium alloy processed via multi-directional forging (MDF) at room temperature.
Mehmet Şahbaz, Sinan Nalkıran
doaj +2 more sources
Strength–Ductility Synergy in Biodegradable Mg-Rare Earth Alloy Processed via Multi-Directional Forging [PDF]
In this study, a biodegradable Mg-Zn-Nd-Gd alloy was processed via multi-directional forging (MDF) to evaluate its microstructural evolution, mechanical performance, and corrosion behavior. Electron backscattered diffraction (EBSD) analysis was conducted
Faseeulla Khan Mohammad +5 more
doaj +2 more sources
Severe plastic deformation (SPD) was carried out on AZ80 alloy by high-pass multi-directional forging (MDF). Results showed that AZ80 alloy was effectively refined through MDF, and average grain size was refined to 0.73 µm after 24 passes of forging. Its
Jinlong Zhang +5 more
doaj +3 more sources
The effect of artificial aging after multi-directional forging of supersaturated AA2024 [PDF]
The primary objective of this study is to determine the most effective solution treatment and aging temperature for AA2024 aluminum alloy to achieve superior mechanical properties.
Mohadeseh Rashidi +2 more
doaj +2 more sources
A newly proposed multi-directional forging (MDF) was successfully applied to a commercially pure titanium (CP Ti). Severe plastic deformation would result in significant and complex changes of microstructure and mechanical properties, so microstructure ...
Zhanguang Zheng +4 more
doaj +3 more sources
Microstructural evolution and mechanical behavior of pearlitic steel under multi-directional forging
The mechanical behavior and the microstructural evolution of a pearlitic SAE 1080 steel were analyzed along 12 Multi-Directional Forging (MDF) cycles at room temperature and strain amplitude Δε ≈ 0.30 (MDF0.30). The resulting cumulative strain flow curve
Nayara Aparecida Neres da Silva +4 more
doaj +3 more sources
Effect of Multi-Directional Forging on the Microstructure and Mechanical Properties of β-Solidifying TiAl Alloy [PDF]
Fantao Kong, Tiewei Xu, Qianqian Wu
exaly +2 more sources
Microstructural Evolution in Large-Section Plastic Mould Steel during Multi-Directional Forging
To obtain excellent mechanical properties from large cross-sections of plastic mould steel (SDP1), we conducted multi-directional forging (MDF) to control the microstructure of ingots. To investigate the microstructural evolution of SDP1 steel during MDF,
Xuan Chen +6 more
doaj +1 more source
Severe Plastic Deformation (SPD) leads to grain refinement and strengthening of metals. Among the many SPD processing methods, Multi-Directional Forging (MDF) is the only one where in-situ material stress–strain curves can be obtained. These are adequate
N.G.S. Almeida +4 more
doaj +1 more source