Analysis on Machining Performance of Nickel-Base Superalloy by Electrochemical Micro-milling with High-Speed Spiral Electrode [PDF]
As one of the most promising micro-machining methods, electrochemical micro-machining is widely used in the field of metal micro-structures. The electrochemical micro-milling on Nickel-base superalloy by using high-speed spiral electrode was studied in ...
Yong Liu +3 more
doaj +2 more sources
Influence of Grain Orientation Distribution on the High Temperature Fatigue Behaviour of Notched Specimen Made of Polycrystalline Nickel-Base Superalloy [PDF]
Two different material batches made of random and textured orientated polycrystalline nickel-base superalloy René80 were investigated under isothermal low cycle fatigue tests at 850 °C for a notched specimen geometry.
Benedikt Engel +3 more
doaj +2 more sources
High‐Throughput Data Generation and Transfer Learning Enabled Microstructure‐Property Integrated Design of Nickel‐Based Powder Metallurgy Superalloy [PDF]
An integrated transfer learning framework integrates CALPHAD simulations, diffusion‐multiple experiments, and literature data to predict long‐term microstructural stability and short‐term mechanical properties of Ni‐based powder metallurgy superalloys. Based on these model predictions, a high‐performance, low‐density alloy, USTB‐PM750, is designed from
Zixin Li +8 more
wiley +2 more sources
Absence of dynamic strain aging in an additively manufactured nickel-base superalloy [PDF]
Detrimental serrated plastic flow via dynamic strain aging (DSA) in conventionally processed nickel superalloys usually occurs during high temperature deformation.
Allison M. Beese +3 more
doaj +2 more sources
Development of Coatings for Gas Turbines Burning Biomass and Waste-Fuels [PDF]
Worldwide, carbon dioxide emission reductions are in progress following the Kyoto Protocol implementation programme to mitigate climate change. More stringent reductions are expected to follow the present programme which ends in 2012.
Bradshaw, A.
core +7 more sources
Investigation of delamination mechanisms during a laser drilling on a cobalt-base superalloy [PDF]
Temperatures in the high pressure chamber of aircraft engines are continuously increasing to improve the engine efficiency. As a result, constitutive materials such as cobalt and nickel-base superalloys need to be thermally protected.
SCHNEIDER, Matthieu +8 more
core +1 more source
An investigation into cracking in nickel-base superalloy repair welds [PDF]
The nickel-base superalloy Rene 80 is considered very susceptible to liquation and strain-age cracking. Material in the solutionised condition is welded using the Cold Metal Transfer, or CMT process (with ductile filler alloy) and autogenously using a
Colegrove, Paul A. +3 more
core +1 more source
Influence of coating on the thermal resistance of a Ni-Based superalloy [PDF]
In this paper, the influence of M-CrAlY polycrystalline coating on the thermal fatigue behavior of a Nickel-base superalloy has been investigated. A special device using a rotating bending machine and two thermal sources has been used to perform thermo ...
Stephan, Nicolas +2 more
core +1 more source
Nickel-Base Superalloy Precipitation - Superalloy Lecture 11
This set of lectures is on "Nickel-Base Superalloy Precipitation" for the Superalloys & High Performance Materials course part 11. This part of the course was taught by Dr Alec Davis at The University of Manchester in 2021.
Materials Engineering +1 more
core +1 more source
Liquation and post-weld heat treatment cracking in Rene 80 laser repair welds [PDF]
An extensive experimental study on a nickel-based superalloy, Rene 80 using autogenous laser welding has been undertaken to determine the effect of the process parameters and weld bead geometry on cracking in the as-welded and post- weld heat treated ...
Colegrove, Paul A. +7 more
core +1 more source