Results 31 to 40 of about 4,091,571 (176)

Influence of Scan Strategies in Electron Beam Powder Bed Fusion on Solidification, Microstructure, and High‐Temperature Compressive Properties of γ′‐Strengthened Inconel 738LC

open access: yesAdvanced Engineering Materials, EarlyView.
Experiments and thermophysical simulations were conducted to investigate the electron beam powder bed fusion electron beam (PBF‐EB/M) process for the γ′‐strengthened nickel‐based superalloy Inconel 738LC. The results demonstrate the impact of process‐induced microstructural variations on high‐temperature mechanical behavior, providing a basis for ...
Jan Niklas Petenati   +11 more
wiley   +1 more source

High‐Temperature Phase Transformation in a V‐9Si‐6.5B Alloy: The Kinetic and Crystallographic Pathway From V5SiB2 to V8SiB4

open access: yesAdvanced Engineering Materials, EarlyView.
In situ synchrotron high‐energy X‐ray diffraction reveals the real‐time high‐temperature phase evolution of a ternary V‐9Si‐6.5B alloy. The study uncovers a kinetically delayed V5SiB2 → V8SiB4 transformation governed by massive structural and chemical barriers.
Zahra Sabeti   +4 more
wiley   +1 more source

Thermodynamic Study on Denitrification and TiN Precipitation in IN718 Nickel Base Superalloy Melt [PDF]

open access: yesTeshugang
Low nitrogen content can control the formation of TiN inclusions, thereby improving the metallurgical quality and comprehensive performance of nickel based high-temperature alloys.
Luo Xiaoyu   +3 more
doaj   +2 more sources

Microstructure Modification of Additively Manufactured Mo–9Si–8B by Annealing and Its Effects on High‐Temperature Mechanical Properties

open access: yesAdvanced Engineering Materials, EarlyView.
Postbuild annealing systematically modifies the phase fractions and morphology of EB‐PBF processed Mo–9Si–8B. Quantitative microstructure–property correlations reveal how controlled phase evolution enhances high‐temperature compressive strength and creep resistance.
Christopher Schmidt   +5 more
wiley   +1 more source

Processing and Characterization 43Ni-14Cr Nickel-Iron Base Superalloy

open access: yesHigh Temperature Materials and Processes, 2012
Nickel-Iron based superalloy (43Ni-14Cr, wt%) is used as high temperature material in space based transportation systems. It retains its high strength (>100 MPa) upto 800°C alongwith good cryogenic properties, hot corrosion ...
Gupta R. K.   +2 more
doaj   +1 more source

Non‐Additive Criteria Assessment in Sustainability Evaluation of High Entropy Alloys: A Toxicity‐Weighted Framework

open access: yesAdvanced Engineering Materials, EarlyView.
Sustainability assessment requires methodologies that appropriately distinguish between additive and non‐additive material properties. A toxicity‐weighted scoring system is developed and applied that accounts for the disproportionate influence of highly toxic constituents through nonlinear weighting functions, providing more realistic estimates than ...
Seth Mehalic   +2 more
wiley   +1 more source

High‐Entropy Alloy Interlayers Toward Advanced Joining for High‐Performance Structural Applications: Current Progress and Emerging Challenges

open access: yesAdvanced Engineering Materials, EarlyView.
HEA interlayers offer a versatile route for joining high‐performance structural materials. Their compositional and structural design regulates interfacial reactions, suppresses brittle IMCs, and improves metallurgical bonding. Sandwich interlayers further integrate defect healing with precipitation strengthening, enabling improved strength–ductility ...
Lin Yuan   +4 more
wiley   +1 more source

High-temperature creep of single-crystal nickel-based superalloy : microstructural changes and effects of thermal cycling [PDF]

open access: yes, 2011
Creep tests were performed on MC2 single crystal superalloy at 950°C/200 MPa and 1150°C/80 MPa under isothermal and thermal cycling conditions with a tensile axis along the [0 0 1] direction. It was found that the thermal cycles strongly affect the creep
Eric Andrieu   +6 more
core   +1 more source

Supporting AI Readiness Through Digital Workflows in Materials Science

open access: yesAdvanced Engineering Materials, EarlyView.
Digitalization drives innovation in materials science by connecting data silos and turning heterogeneous processes into reusable research pipelines. Across 13 MaterialDigital projects, digital workflows reveal complementary pathways toward AI‐ready materials research, founded on structured data, persistent artifacts, executable orchestration, and ...
Marian Bruns   +67 more
wiley   +1 more source

Identification of influent factors on surface integrity in nickel-base superalloy drilling [PDF]

open access: yes, 2010
For the critical rotating components in aeronautical industry, the metallurgical quality achieved after machining conditions could determine their mechanical behaviour in fatigue. To guarantee this quality, the tools, materials and cutting conditions are
Dutilh, Vincent   +4 more