Results 21 to 30 of about 4,091,571 (176)
Pore annihilation was investigated in the single-crystal nickel-base superalloy CMSX-4. HIP tests at 1288 °C/103 MPa were interrupted at different times, then the specimens were investigated by TEM, metallography and density measurements. The kinetics of
Epishin Alexander I. +4 more
doaj +1 more source
Nickel base superalloys are hi-tech materials intended for high temperature applications. This property owns a complex microstructure formed by matrix of Ni and variety of precipitates.
Michal Jambor +4 more
doaj +2 more sources
Vacuum brazing of K465 superalloy was carried out by using Co45NiCrWB cobalt-base filler metal at 1220 ℃ for different holding time, and the joint clearance was 0.5 mm pre-filled with FGH95 nickel-base superalloy powder.
PAN Hui, ZHAO Haisheng
doaj +1 more source
Electrochemical Noise Analysis of Nickel Based Superalloys in Acid Solutions
In this paper we study the corrosion behavior of nickel-based superalloys (Inconel 690, Inconel 718, Incoloy 800, Incoloy 825), compared with commercial steels (carbon Steel 1018 and stainless steel 304), in acid (10% H2SO4 and 10 % CH3COOH) and H2O at ...
C. Gaona-Tiburcio +7 more
doaj +1 more source
The Structure and Stability of High Temperature Intermetallic Phases for Application within Coating Systems [PDF]
The reduction of noise and emissions is becoming increasingly important in civil aircraft jet engines as well as requirements for reduced fuel consumption and improved efficiency.
Roberts, Tracey
core +6 more sources
In this work, we investigate the effect of hot isostatic pressing on the intermediate temperature tensile property of nickel-base single crystal superalloy.
Weidong Xuan +6 more
doaj +1 more source
The control of titanium and aluminium in nickel-base superalloy with high titanium and low aluminium during the electroslag remelting (ESR) process has not been resolved well so far.
Jianpeng Tan +5 more
doaj +1 more source
An assessment of the effects of microstructure on room temperature fatigue crack initiation and short crack propagation in a Ni-base superalloy is presented.
Pang, H.T., Reed, P.A.S.
core +1 more source
In this study, the third-generation rhenium containing single crystal superalloy was brazed by mixed powder filler, in which the mixed powder filler was consisted of nickel-based powder filler and the superalloy powder with the same composition of the ...
LI Kexin +8 more
doaj +1 more source
Tensile Behavior of Long-term Aged Nickel-base Superalloy
The microstructural change of directionally solidified nickel-base superalloy which was aged at 900 °C for 1500 hours and tensile behavior at different temperatures were investigated by scanning electron microscope (SEM) and transmission electron ...
Xia P. C., Chen F. W., Xie K., Yu J. J.
doaj +1 more source