Results 51 to 60 of about 15,457 (271)
Deformation‐Induced Formation of Stray Grains in Additive Manufacturing of Single Crystals
Stray grain formation severely limits the additive manufacturing of single‐crystal alloys. By integrating in situ synchrotron techniques, ex situ characterization, and multi‐scale multi‐physics modeling, the authors reveal that stray grains originate from dislocations at the solid‐liquid interface, rather than thermal supercooling in conventional ...
Dongsheng Zhang +11 more
wiley +1 more source
Biaxial constitutive equation development [PDF]
In developing the constitutive equations an interdisciplinary approach is being pursued. Specifically, both metallurgical and continuum mechanics considerations are recognized in the formulation.
Jordan, E. H., Walker, K. P.
core +1 more source
Advanced burner-rig test for oxidation-corrosion resistance evaluation of MCrAlY/superalloys systems [PDF]
Protective coatings are used on gas turbine components to enable them to survive in engine-operating conditions. This study presents a recently developed cyclic burner-rig test that is used to simulate helicopter engine conditions and to assess the ...
Andrieu, Eric +3 more
core +3 more sources
This work presents a novel generative artificial intelligence (AI) framework for inverse alloy design through operations (optimization and diffusion) within learned compact latent space from variational autoencoder (VAE). The proposed work addresses challenges of limited data, nonuniqueness solutions, and high‐dimensional spaces.
Mohammad Abu‐Mualla +4 more
wiley +1 more source
Clean recycling of spent nickel-based single-crystal superalloy by molten magnesium
Nickel-based single-crystal superalloys are designed for extreme conditions due to their superior corrosion and creep resistance properties. However, these pose challenges in the subsequent recycling after reaching their end-of-life. Molten magnesium (Mg)
Hao Li +6 more
doaj +1 more source
The isothermal oxidation behavior of a second generation Ni-base single crystal superalloy was investigated in air at 1000°C and 1100°C. The microstructures of the oxide morphology and the crosssection area of the specimens after oxidation were analyzed ...
Fahamsyah H. Latief +3 more
doaj +1 more source
Feature from recent image foundation models (DINOv2) are useful for vision tasks (segmentation, object localization) with little or no human input. Once upsampled, they can be used for weakly supervised micrograph segmentation, achieving strong results when compared to classical features (blurs, edge detection) across a range of material systems.
Ronan Docherty +2 more
wiley +1 more source
SciLitMiner: An Intelligent System for Scientific Literature Mining and Knowledge Discovery
SciLitMiner is an intelligent system that federately ingests scientific literature, filters it using advanced information retrieval methods, and applies retrieval‐augmented generation tailored to scientific domains. Demonstrated on creep deformation in γ‐TiAl alloys, SciLitMiner provides a controlled workflow for systematic knowledge discovery and ...
Vipul Gupta +3 more
wiley +1 more source
Advanced materials research for long-haul aircraft turbine engines [PDF]
The status of research efforts to apply low to intermediate temperature composite materials and advanced high temperature materials to engine components is reviewed.
Blankenship, C. P., Signorelli, R. A.
core +1 more source
Cyclic thermogravimetry of TBC systems [PDF]
The previously developed cyclic thermogravimetry analysis (CTGA) method is applied to the cyclic oxidation at 1100 °C of ZrO2–Y2O3/NiPtAl or NiCoCrAlYTa/single crystal nickel-base AM3 superalloy TBC systems.
Monceau, Daniel +2 more