Results 91 to 100 of about 9,930 (219)
A 3D Analysis of Dendritic Solidification and Mosaicity in Ni-Based Single Crystal Superalloys. [PDF]
Scholz F +5 more
europepmc +1 more source
Isothermal and bithermal thermomechanical fatigue behavior of a NiCoCrAlY-coated single crystal superalloy [PDF]
Specimens of single crystal PWA 1480 with group of zone axes (100) orientation, bare, or with NiCoCrAlY coating PWA 276, were tested in low cycle fatigue (LCF) at 650, 870, and 1050 C, and in simplified bithermal thermomechanical fatigue (TMF) tests ...
Gabb, T. P., Gayda, J., Miner, R. V.
core +1 more source
Elastic response of zone axis (001)-oriented PWA 1480 single crystal: The influence of secondary orientation [PDF]
The influence of secondary orientation on the elastic response of a zone axis (001)-oriented nickel-base single-crystal superalloy, PWA 1480, was investigated under mechanical loading conditions by applying finite element techniques.
Abdul-Aziz, Ali +2 more
core +1 more source
Optimizing carbon content is critical for the design of Ni-based single-crystal superalloys, particularly for high-temperature applications. This study systematically investigated the influence of carbon on the solidification behavior and phase evolution
Xiaoyu Song +10 more
doaj +1 more source
Micromechanics of cyclic deformation in SSME turbopump blade materials [PDF]
Current and candidate Space Shuttle Main Engine (SSME) turbopump blade materials are anisotropic, both in their elastic and plastic response. The major objective is to characterize the plastic deformation behavior of a typical single crystal nickel-base ...
Antolovich, Stephen D. +1 more
core +1 more source
nickel-based single crystal superalloy [PDF]
null Re同Cr和Co元素共偏聚于尖端区域 +1 more
openaire +1 more source
It is hard to improve the oxidation resistance property of single-crystal (SC) Ni-based superalloys except for alloying design since monocrystalline lacks defects such as grain boundaries that are beneficial for antioxidant elemental diffusion. This work
Boxuan Du +9 more
doaj +1 more source
Influence of composition on the microstructure and mechanical properties of a nickel-base superalloy single crystal [PDF]
The effects of cobalt, tantalum, and tungsten contents on the microstructure and mechanical properties of single crystal Mar-M247 were investigated. Elevated temperature tensile and creep-rupture properties of 001 oriented single crystals were related ...
Ebert, L. J., Nathal, M. V.
core +1 more source
Nickel-based superalloys are important structural materials in turbine engines and gas turbines,but their conventional fabrication processes are complex,costly and have poor raw-material-utilization rate.
QIAN Huxiao +4 more
doaj +1 more source
The mechanisms of dislocation/precipitate interaction were studied by means of discrete dislocation dynamics within a multiscale approach. Simulations were carried out using the discrete continuous method in combination with a fast Fourier transform ...
Capolungo, L. +5 more
core +1 more source