Results 111 to 120 of about 9,930 (219)
High-performance brazing of single crystal superalloys with Ni-Cr-Ta filler material
High-performance joining especially brazing has been highly expected in the manufacture or maintenance of single crystal blades. In this paper, a Ni-40Cr-10Ta (at.%) alloy was developed as filler material for single crystal superalloys.
Zhenqian Lang +6 more
doaj +1 more source
Composition rules of Ni-base single crystal superalloys and its influence on creep properties via a cluster formula approach. [PDF]
Chen C, Wang Q, Dong C, Zhang Y, Dong H.
europepmc +1 more source
The traditional design of single-crystal superalloys relies heavily on trial-and-error experimentation, which is time-consuming and costly. Here, we present an intelligent alloy design strategy that integrates natural language processing (NLP) and ...
Jian Yao +13 more
doaj +1 more source
Single crystal superalloy turbine rotor blade is one of the core hot-end components of the aero-engine, which has a decisive role in the thrust and performance of the aero-engine.
QIN Renyao +5 more
doaj +1 more source
Fatigue damage modeling for coated single crystal superalloys [PDF]
A high temperature, low-cycle fatigue life prediction method for coated single crystal nickel-base superalloys is being developed. The method is being developed for use in predicting crack initiation life of coated single crystal turbine airfoils ...
Nissley, David M.
core +1 more source
Thermal fatigue durability for advanced propulsion materials [PDF]
A review is presented of thermal and thermomechanical fatigue (TMF) crack initiation life prediction and cyclic constitutive modeling efforts sponsored recently by the NASA Lewis Research Center in support of advanced aeronautical propulsion research.
Halford, Gary R.
core +1 more source
On Thermomechanical Fatigue of Single-Crystal Superalloys
Thanks to their excellent mechanical and chemical properties at temperatures up to 1000 °C, nickel-based superalloys are used in critical components in high-temperature applications such as gas turbines and aero engines. One of the most critical components in a gas turbine is the turbine blade, and to improve the creep and fatigue properties of this ...
openaire +4 more sources
Influence of a magnetic field during directional solidification of MAR-M 246 + Hf superalloy [PDF]
An area that has been almost totally overlooked in the optimization of properties in directionally solidified superalloys is the control of microstructural features through the application of a magnetic field during solidification.
Alter, Wendy +2 more
core +1 more source
Prospects for Ductility and Toughness Enhancement of Nial by Ductile Phase Reinforcement [PDF]
The use of NiAl as a structural material has been hindered by the fact that this ordered intermetallic does not exhibit significant tensile ductility or toughness at room temperature.
Gibala, R. +3 more
core +1 more source
Thermal fatigue and oxidation data for directionally solidified MAR-M 246 turbine blades [PDF]
Thermal fatigue and oxidation data were obtained for 11 plasma spray coated and 13 uncoated directionally solidified and single crystal MAR-M 246 blades.
Hill, V. L., Humphreys, V. E.
core +1 more source