Results 41 to 50 of about 64,035 (272)

A Workflow to Accelerate Microstructure‐Sensitive Fatigue Life Predictions

open access: yesAdvanced Engineering Materials, EarlyView.
This study introduces a workflow to accelerate predictions of microstructure‐sensitive fatigue life. Results from frameworks with varying levels of simplification are benchmarked against published reference results. The analysis reveals a trade‐off between accuracy and model complexity, offering researchers a practical guide for selecting the optimal ...
Luca Loiodice   +2 more
wiley   +1 more source

Influence of Environment on Creep Properties of MC2 Single Crystal Superalloy at 1150°C [PDF]

open access: yes, 2004
In order to reveal the effect of oxidation on thin blade walls, a new machine allowing tests up to 1250°C under controlled atmosphere has been designed.
Andrieu, Eric   +4 more
core   +1 more source

Elinvar Materials: Recent Progress and Challenges

open access: yesAdvanced Engineering Materials, EarlyView.
Elinvar materials, exhibiting temperature‐invariant elastic modulus, are critical for precision instruments and emerging technologies. This article reviews recent progress in the field, with a focus on the anomalous thermoelastic behavior observed in key material systems.
Wenjie Li, Yang Ren
wiley   +1 more source

Silicon-slurry/aluminide coating [PDF]

open access: yes, 1983
A low cost coating protects metallic base system substrates from high temperatures, high gas velocity ovidation, thermal fatigue and hot corrosion and is particularly useful fo protecting vanes and blades in aircraft and land based gas turbine engines. A
Deadmore, D. L., Young, S. G.
core   +1 more source

Direct Laser Fabrication of a Gas Turbine Engine Component - Microstructure and Properties - Part I [PDF]

open access: yes, 1998
This paper presents the development of a new technique for the production of abrasive turbine blade tips by direct laser processing. This superalloy cermet component is an integral part of the low pressure turbine sealing system in a demonstrator ...
Beaman, Joseph J.   +6 more
core   +1 more source

Thermomechanical Fatigue and Creep–Fatigue Interaction of Inconel 718 Additively Manufactured by Laser Beam Powder Bed Fusion

open access: yesAdvanced Engineering Materials, EarlyView.
Thermomechanical fatigue tests of laser beam powder bed fusion (PBF‐LB) Inconel 718 show that the additively manufactured material reaches almost the lifetimes of conventionally‐rolled material under no‐dwell conditions. Introducing dwell times at the maximum temperature markedly reduces the lifetimes due to pronounced grain boundary sliding associated
Stefan Guth   +6 more
wiley   +1 more source

Hot Ductility Loss in a Fe-Ni-Based Superalloy

open access: yesMetals, 2015
High temperature tensile tests have been conducted on samples of a Fe-Ni based superalloy, Incoloy A-286, and significant ductility loss has been observed at 1220 °C.
Chen-Wei Li   +3 more
doaj   +1 more source

Temperature evolution and grain defect formation during single crystal solidification of a blade cluster [PDF]

open access: yesChina Foundry, 2017
In order to investigate the asymmetry of thermal conditions during directional solidification, the temperature evolution and correspondingly developed undercooling in a simplified single crystal blade cluster were numerically simulated.
De-xin Ma, Fu Wang, Qiang Wu
doaj   +1 more source

Study of the Creep Behavior of Nickel-Based Single Crystal Superalloy Micro Specimens with Dimensional Effects

open access: yesCrystals, 2022
Nickel-based single-crystal superalloys are widely used in aeroengine hot-end components, owing to their unique crystal structure and outstanding high-temperature mechanical properties.
Wangjiao Xiong   +7 more
doaj   +1 more source

Heat treatment for superalloy [PDF]

open access: yes, 1987
A cobalt-free nickel-base superalloy composed of in weight % 15 Cr-5 Mo-3.5 Ti-4 Al-0.07 (max) C-remainder Ni is given a modified heat treatment.
Harf, Fredric H.
core   +1 more source