Results 51 to 60 of about 355,851 (216)
Figures for "Microstructure and Texture Development during Solid Consolidation Recycling of Ti-6Al-4V" [PDF]
Figures showing the results of the microstructural evolution of recycled Ti-6Al-4V sample from machining chips using ECAP method.They are associated with the article "Microstructure and Texture Development during Solid Consolidation Recycling of Ti-6Al ...
Qi (Alex) Shi (7124834) +3 more
core +1 more source
SURFACE CHARACTERIZATION AND CYTOTOXICITY ANALYSIS OF THE TITANIUM ALLOYS FOR DENTISTRY
Three methods of treating the Ti and Ti-6Al-4V alloy surface used as dental implants have been tried both to increase the corrosion resistance and to create diffusion barriers, which prevent the release of toxic ions in the body, at the separation ...
Paula Argentina JIMAN +7 more
doaj +1 more source
Influence of various process conditions on surface finishes induced by the direct metal deposition laser technique on a Ti–6Al–4V alloy [PDF]
The direct metal deposition (DMD) with laser is a free-form metal deposition process for manufacturing dense pieces, which allows generating a prototype or small series of near net-shape structures. One of the most critical issues is that produced pieces
GORNY, Cyril +7 more
core +1 more source
The corrosion resistance of titanium alloy poses a crucial challenge, significantly affecting its prospect for service and application. The present study aimed to investigate the corrosion resistance of Ti-6Al-4V ELI alloys with varying surface roughness
Han Wang +5 more
doaj +1 more source
Sol–gel‐derived ZnO–rGO hybrid nanoparticles enable Al7075 powder‐metallurgy composites to achieve concurrent gains in hardness and thermal conductivity while markedly lowering friction and wear. The hybrid architecture couples ZnO‐based load support with rGO‐assisted lamellar sliding and heat spreading, revealing a promising route toward lightweight ...
Bunyamin Aksakal +3 more
wiley +1 more source
Coupling mechanisms of static and dynamic loads during the ultrasonic impact strengthening of Ti-6Al-4V [PDF]
The ultrasonic impact-strengthening technology was used to effectively improve the fatigue resistance of the key components, which could be attributed to the association of static and dynamic impact loads.
Xuming Zha (20258079) +6 more
core
Study on selective laser melting and heat treatment of Ti-6Al-4V alloy
The effects of process parameters of laser additive manufacturing (laser power, scanning speed, scanning direction) and heat treatment on the microstructure and properties of Ti-6Al-4V titanium alloy forming parts were studied under coaxial powder ...
Zhechao Fan, Hongwei Feng
doaj +1 more source
Additive manufacturing provides an appealing means to process titanium alloy parts with new levels of conformability, complexity, and weight reduction.
Jonathan W. Pegues +7 more
semanticscholar +1 more source
X‐ray computed tomography reveals how process‐induced defects evolve from green to sintered states in Fused Filament Fabrication (FFF)‐manufactured 17‐4PH stainless steel. Internal porosity, weakest cross‐sections, and fracture locations show strong correlation with tensile performance, demonstrating the potential of computed tomography (CT)‐based ...
György Ledniczky +3 more
wiley +1 more source
Influence of Rotational Speed in the Friction Surfacing of Titanium Grade 1 on Ti-6Al-4V [PDF]
Titanium Grade 1 was deposited on Ti-6Al-4V, 2 mm thickness, by Friction Surfacing. The process parameters were rotational speed, deposition speed and consumption rate.
Jorge Fernandez dos Santos (4791864) +4 more
core +1 more source